Dissolution behavior of Mg-Al-Cu and Mg-Zn-Cu alloys for fracturing ball applications: A comparative investigation
Source abstract
Abstract
As-extruded Mg-6Al-1Zn-0.5Cu and Mg-6Zn-0.5Cu alloys with comparable strength were prepared, and their dissolution behaviors in KCl solutions with different Cl − concentrations were investigated for use as fracturing balls. The results of electrochemical and immersion tests consistently demonstrated that Mg-6Al-1Zn-0.5Cu alloy exhibited superior corrosion resistance across all tested environments. Specifically, in 1 wt.% KCl, it displayed a lower corrosion current density (1.28 × 10 –4 A/cm 2 ) and weight loss (19.2 mg/cm 2 /d). This superior performance was attributed to its finer grains, smaller galvanic potential differences, and more stable oxide film. Furthermore, a strong dependence on Cl − concentration was established, with higher Cl − levels accelerating corrosion. This research provides insight into the microstructure-corrosion relationship and offers guidance for material selection, recommending Mg-6Al-1Zn-0.5Cu alloy for fracturing balls across a wide range of Cl − environments during the initial stage of hydraulic fracturing.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Xi’an Shiyou University
Funding
National Natural Science Foundation of China · Graduate Innovation Fund Project of Xi’an Shiyou University
References (41)
Show source-provided references
1. 10.1016/j.ngib.2018.11.00210.1016/j.ngib.2018.11.002 ↗
2. 10.1016/j.jpcs.2020.10949910.1016/j.jpcs.2020.109499 ↗
3. 10.1016/j.matdes.2014.12.05010.1016/j.matdes.2014.12.050 ↗
4. 10.1016/j.jma.2019.11.01010.1016/j.jma.2019.11.010 ↗
5. 10.3390/met1303044610.3390/met13030446 ↗
6. 10.1016/j.petrol.2011.11.00210.1016/j.petrol.2011.11.002 ↗
7. 10.1016/j.wear.2020.20355910.1016/j.wear.2020.203559 ↗
8. 10.1007/s12206-017-0115-310.1007/s12206-017-0115-3 ↗
9. 10.1016/j.petrol.2017.03.03510.1016/j.petrol.2017.03.035 ↗
10. 10.1016/j.jma.2025.01.01110.1016/j.jma.2025.01.011 ↗
11. 10.1016/j.jallcom.2022.16499510.1016/j.jallcom.2022.164995 ↗
12. 10.1016/j.mtcomm.2025.11210010.1016/j.mtcomm.2025.112100 ↗
13. 10.1080/21663831.2025.249389810.1080/21663831.2025.2493898 ↗
14. 10.1016/j.msea.2008.12.02910.1016/j.msea.2008.12.029 ↗
15. 10.3390/met1201008410.3390/met12010084 ↗
16. Su J, Guo F, Cai HS, et al. Effect of solid solution amount of Zn on microstructure of Mg-Zn-Y alloy. Rare Met Mater Eng 2019; 48: 2179–2184.
17. 10.1016/j.corsci.2017.08.01410.1016/j.corsci.2017.08.014 ↗
18. 10.1007/s11665-016-2207-010.1007/s11665-016-2207-0 ↗
19. 10.1016/j.jmst.2025.04.00710.1016/j.jmst.2025.04.007 ↗
20. 10.2320/matertrans.L-M202083910.2320/matertrans.L-M2020839 ↗
21. 10.1016/j.jallcom.2017.12.25710.1016/j.jallcom.2017.12.257 ↗
22. 10.1002/maco.20170982710.1002/maco.201709827 ↗
23. 10.1016/j.matlet.2017.02.02410.1016/j.matlet.2017.02.024 ↗
24. 10.1016/S1003-6326(14)63101-010.1016/S1003-6326(14)63101-0 ↗
25. 10.1016/j.jma.2024.03.01610.1016/j.jma.2024.03.016 ↗
26. 10.1016/j.jma.2025.06.00210.1016/j.jma.2025.06.002 ↗
27. 10.1016/j.jma.2021.09.01810.1016/j.jma.2021.09.018 ↗
28. 10.1016/j.msea.2022.14300210.1016/j.msea.2022.143002 ↗
29. Zhao YC, Yao H, Zhang XY, et al. Microstructure and mechanical properties of Mg-Zn-Mn alloys with different Y contents after solution treatment. Trans Mater Heat Treat 2026; 47: 70–77.
30. Jiang AX, You ZY, Sun CL, et al. Effects of T6 treatment on microstructure and properties of Mg-Zn-Ce alloys with different Zn contents. Spec Cast Nonferr Alloys 2026; 46: 525–531.
31. Jiang FS, Li L, Xu P, et al. Effect of trace ca on microstructure and corrosion behavior of mg-zn-al alloy. The Chinese Journal of Nonferrous Metals 2025; 35: 3441–3453.
32. Wang DW Zhou R Yang YJ et al. Mechanisms for synergistically enhanced mechanical properties and corrosion resistance in Mg-Al-Sn alloys. Trans Nonferr Met Soc China. https://link.cnki.net/urlid/43.1239.TG.20250721.1628.018.
33. 10.1016/j.corsci.2009.10.01610.1016/j.corsci.2009.10.016 ↗
34. 10.1016/j.actbio.2011.11.01410.1016/j.actbio.2011.11.014 ↗
35. 10.1080/02670836.2023.217389310.1080/02670836.2023.2173893 ↗
36. 10.1016/j.jmst.2021.05.01010.1016/j.jmst.2021.05.010 ↗
37. 10.1016/j.jma.2022.06.01610.1016/j.jma.2022.06.016 ↗
38. 10.3390/met805032310.3390/met8050323 ↗
39. 10.1016/j.corsci.2006.05.03310.1016/j.corsci.2006.05.033 ↗
40. 10.1016/j.apgeochem.2024.10603210.1016/j.apgeochem.2024.106032 ↗
41. 10.1016/j.cemconcomp.2025.10603210.1016/j.cemconcomp.2025.106032 ↗