journal article·2026-07-14

Dynamic mechanical properties and microstructure evolution of Mg-6Zn-(2Gd)-0.6Zr magnesium alloys

Yifan Zhang, Mingfeng Liu, Zhi Wang, Xudong Du, Le Zhou, Feng Wang, Pingli Mao

Publisher page

Abstract

In this study, Mg-6Zn-(2Gd)-0.6Zr alloys were fabricated by the extrusion-shearing process. Dynamic compression experiments were conducted using a split Hopkinson pressure bar (SHPB) at strain rates from 800 to 2500 s −1 . The influence of strain rates on microstructural evolution was systematically characterized. The results showed that the average grain sizes are refined from 17.4 µm in the Mg-6Zn-0.6Zr alloy to 3.6 µm in the Mg-6Zn-2Gd-0.6Zr alloy. The peak flow stresses of the two alloys increase monotonically with strain rates, exhibiting strain rate strengthening. The tensile twinning is the main deformation mechanism of dynamic compression. Meanwhile, most activated tensile twin variants follow Schmid's law, while twin nucleation with lower Schmid factors is due to strain accommodation between adjacent grains.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · High-Velocity Impact and Material Behavior · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Shenyang University of Technology

Key Laboratory of Magnesium Alloys and the Processing Technology of Liaoning Province, Shenyang, China

Key Laboratory of Lightweight Forming Technology for Automobile Components of Shenyang, Shenyang, China

Automobile Lightweight Technology Professional Innovation Center of Liaoning Province, Tieling, China

Funding

Doctoral Research Initiation Fund Program of the Natural Science Foundation of Liaoning Province · Applied Basic Research Program of the Science and Technology Plan of Liaoning Province · Liaoning Provincial Science and Technology Program Joint Project

References (36)

Show source-provided references
1. 10.1016/j.matpr.2020.01.25510.1016/j.matpr.2020.01.255 ↗
2. 10.1016/j.jma.2025.09.01410.1016/j.jma.2025.09.014 ↗
3. 10.1016/j.jma.2019.08.00110.1016/j.jma.2019.08.001 ↗
4. 10.1016/j.matpr.2020.07.42410.1016/j.matpr.2020.07.424 ↗
5. Viswanadhapalli B, Bupesh Raja VK. Application of magnesium alloys in automotive industry-a review[J]. Emerg Trends Comput Expert Technol 2020; 35: 519–531.
6. 10.1016/S1359-6462(02)00591-210.1016/S1359-6462(02)00591-2 ↗
7. 10.1016/j.actamat.2019.03.02710.1016/j.actamat.2019.03.027 ↗
8. 10.1016/j.ijplas.2023.10352510.1016/j.ijplas.2023.103525 ↗
9. 10.1016/j.msea.2021.14115210.1016/j.msea.2021.141152 ↗
10. 10.1016/j.actamat.2019.07.04610.1016/j.actamat.2019.07.046 ↗
11. 10.1016/j.jma.2022.09.00310.1016/j.jma.2022.09.003 ↗
12. 10.1016/S0921-5093(01)01297-710.1016/S0921-5093(01)01297-7 ↗
13. 10.1016/j.msea.2020.13980110.1016/j.msea.2020.139801 ↗
14. Livescu V, Cady CM, Cerreta EK, et al. The high strain rate deformation behavior of high purity magnesium and AZ31B magnesium alloy[J]. Ess Read Magnes Technol 2016: 375–380.
15. 10.3390/ma1401008710.3390/ma14010087 ↗
16. 10.1016/j.actamat.2020.09.08210.1016/j.actamat.2020.09.082 ↗
17. 10.1007/s11665-020-05162-510.1007/s11665-020-05162-5 ↗
18. 10.1016/j.msea.2019.13864910.1016/j.msea.2019.138649 ↗
19. Malik A, Yangwei W, Huanwu C, et al. Fracture behavior of twin induced ultra-fine grained ZK61 magnesium alloy under high strain rate compression[J]. J Mater Eng Perform 2019; 8: 3475–3486.
20. 10.3390/ma1401008710.3390/ma14010087 ↗
21. 10.1080/14786435.2018.142789610.1080/14786435.2018.1427896 ↗
22. 10.1016/j.msea.2016.12.01510.1016/j.msea.2016.12.015 ↗
23. 10.1016/j.msea.2021.14099410.1016/j.msea.2021.140994 ↗
24. 10.1080/02670836.2019.163058310.1080/02670836.2019.1630583 ↗
25. Wang Z, Liu B, Huang S, et al. Microstructure and mechanical properties of extrusion ZC61 alloys under different dynamic compression loading directions[J]. Mater Today Commun 2022; 30: 103123.
26. 10.1016/j.msea.2018.02.04510.1016/j.msea.2018.02.045 ↗
27. 10.1016/j.ijplas.2017.04.00610.1016/j.ijplas.2017.04.006 ↗
28. 10.1016/j.ijplas.2014.12.00110.1016/j.ijplas.2014.12.001 ↗
29. 10.1016/S1003-6326(20)65315-810.1016/S1003-6326(20)65315-8 ↗
30. 10.1016/j.scriptamat.2010.06.04710.1016/j.scriptamat.2010.06.047 ↗
31. 10.1016/j.msea.2015.03.02010.1016/j.msea.2015.03.020 ↗
32. 10.1016/j.matchar.2020.11069010.1016/j.matchar.2020.110690 ↗
33. 10.1016/j.jmps.2012.06.01510.1016/j.jmps.2012.06.015 ↗
34. 10.1016/j.scriptamat.2006.07.05910.1016/j.scriptamat.2006.07.059 ↗
35. Luster J, Morris MA. Compatibility of deformation in two-phase Ti-Al alloys: dependence on microstructure and orientation relationships[J]. J Mech Phys Solids 1995; 26: 1745–1756.
36. 10.1016/j.matchar.2025.11531310.1016/j.matchar.2025.115313 ↗