journal article·2026-04-28

Influence of varying aluminum contents on the hot ductility of medium manganese steels

Daniel David, Reinhold Schneider, Gerald Klösch, Christof Sommitsch

Publisher page

Abstract

The influence of aluminum nitride (AlN) precipitation on the hot ductility of medium manganese steels was investigated using hot tensile testing, as good hot ductility is essential for continuous casting. A reasonable hot ductility is reached up to 0.04% and at 1.6% aluminum. At 0.04% only few AlN precipitates due to slow kinetics. At 1.6%, coarse AlN precipitates at high temperatures, minimally affecting hot ductility. In contrast, 0.6% aluminum leads to significant ductility loss due to AlN precipitating at γ Fe grain boundaries. At 1% aluminum, higher nitrogen contents only slightly reduce hot ductility. Thus, hot ductility is mainly influenced by AlN precipitation from γ Fe . SEM-EDX analysis confirmed that fine AlN at γ Fe grain boundaries correlate with poor hot ductility.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Microstructure and Mechanical Properties of Steels · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

University of Applied Sciences Upper Austria

Graz University of Technology

voestalpine Stahl Donawitz GmbH, Leoben, Austria

Funding

Österreichische Forschungsförderungsgesellschaft

References (56)

Show source-provided references
1. 10.2355/isijinternational.55.66210.2355/isijinternational.55.662 ↗
2. 10.1007/s11661-012-1402-310.1007/s11661-012-1402-3 ↗
3. 10.3139/105.11038110.3139/105.110381 ↗
4. 10.1002/srin.20200018110.1002/srin.202000181 ↗
5. 10.1016/j.msea.2022.14306710.1016/j.msea.2022.143067 ↗
6. 10.1080/02670836.2021.188275410.1080/02670836.2021.1882754 ↗
7. 10.1515/htm-2021-002010.1515/htm-2021-0020 ↗
8. 10.1016/j.msea.2020.13932110.1016/j.msea.2020.139321 ↗
9. 10.1007/s11661-002-0378-910.1007/s11661-002-0378-9 ↗
10. 10.1080/02670836.2017.132008510.1080/02670836.2017.1320085 ↗
11. 10.1016/j.scriptamat.2021.11392310.1016/j.scriptamat.2021.113923 ↗
12. Gramlich A, Van der Linde C, Ackermann, et al. Effect of molybdenum, aluminium and boron on the phase transformation in 4 wt.–% manganese steels. Results Mater 2020; 8: 1–8.
13. 10.3390/met1307120610.3390/met13071206 ↗
14. 10.1002/srin.20240015910.1002/srin.202400159 ↗
15. 10.1016/j.mser.2020.10059010.1016/j.mser.2020.100590 ↗
16. 10.1016/j.jmrt.2021.08.01910.1016/j.jmrt.2021.08.019 ↗
17. 10.3390/met1203050210.3390/met12030502 ↗
18. 10.1179/imr.1991.36.1.18710.1179/imr.1991.36.1.187 ↗
19. 10.2355/isijinternational.39.83310.2355/isijinternational.39.833 ↗
20. 10.1007/s11665-018-3599-910.1007/s11665-018-3599-9 ↗
21. 10.1080/02670836.2021.188204710.1080/02670836.2021.1882047 ↗
22. 10.1179/174367507X24735910.1179/174367507X247359 ↗
23. 10.1179/mst.1992.8.2.17110.1179/mst.1992.8.2.171 ↗
24. 10.1179/026708309X1252662033827810.1179/026708309X12526620338278 ↗
25. Gontijo M, Hoflehner C, Ilie S, et al. Holding time influence on the hot ductility behavior of a continuously cast low alloy steel. Metals (Basel) 2021; 11: 1–17.
26. 10.2355/isijinternational.33.41310.2355/isijinternational.33.413 ↗
27. 10.2355/isijinternational1966.27.50610.2355/isijinternational1966.27.506 ↗
28. 10.1179/1743284711Y.000000001310.1179/1743284711Y.0000000013 ↗
29. 10.2355/isijinternational1966.25.14910.2355/isijinternational1966.25.149 ↗
30. 10.2355/isijinternational1966.22.18110.2355/isijinternational1966.22.181 ↗
31. 10.1179/1743284715Y.000000012610.1179/1743284715Y.0000000126 ↗
32. Tuling A. The effect of precipitation and microstructure on hot ductility in high Al Nb containing TRIP steels. PhD Thesis University of London UK 2010.
33. 10.1179/mt.1978.5.1.15010.1179/mt.1978.5.1.150 ↗
34. Thomas BG, Brimacombe JK, Samarasekera IV. The formation of panel cracks in steel ingots- A state-of-the-art review. ISS trans 1986; 10: 7–20.
35. 10.1179/mst.1985.1.7.52010.1179/mst.1985.1.7.520 ↗
36. 10.2355/isijinternational1966.24.16910.2355/isijinternational1966.24.169 ↗
37. 10.1179/03071698380329137010.1179/030716983803291370 ↗
38. 10.1179/1743284711Y.000000010910.1179/1743284711Y.0000000109 ↗
39. 10.1179/mst.1998.14.3.22710.1179/mst.1998.14.3.227 ↗
40. 10.2355/isijinternational.49.142410.2355/isijinternational.49.1424 ↗
41. 10.1007/s11663-013-9851-710.1007/s11663-013-9851-7 ↗
42. 10.1179/mst.1991.7.12.110110.1179/mst.1991.7.12.1101 ↗
43. 10.1002/srin.20170034210.1002/srin.201700342 ↗
44. 10.1080/03019233.2020.179154910.1080/03019233.2020.1791549 ↗
45. 10.1016/j.jmrt.2022.03.12210.1016/j.jmrt.2022.03.122 ↗
46. 10.1016/j.jmrt.2019.10.02810.1016/j.jmrt.2019.10.028 ↗
47. 10.1002/srin.20210032310.1002/srin.202100323 ↗
48. 10.1179/mst.1996.12.2.13210.1179/mst.1996.12.2.132 ↗
49. 10.1002/mawe.20240024910.1002/mawe.202400249 ↗
50. 10.1179/174328413X1378982429394810.1179/174328413X13789824293948 ↗
51. 10.1179/026708304X426810.1179/026708304X4268 ↗
52. 10.1179/mst.1993.9.10.90710.1179/mst.1993.9.10.907 ↗
53. Stieben A. Eigenschaften lufthärtender martensitischer Schmiedestähle mit Mangangehalten von 3–10%. PhD Thesis RWTH Aachen Germany 2018.
54. David D, Schneider R, Klösch G, et al. Influence of alloying elements on the transformation behavior of Medium-manganese-steels. NETSUSHORI 2024; 64: 187–192.
55. 10.3139/105.11027310.3139/105.110273 ↗
56. 10.1201/978100305678210.1201/9781003056782 ↗