Insight into the influence of pre-charging hydrogen on mechanical behavior and fracture morphology of X52MS pipeline steel
Source abstract
Abstract
The hydrogen supply pipelines can lead to failure behaviors such as hydrogen-induced cracking and reduced plasticity when it is exposed to hydrogen-containing media during service, which is related to the migration feature of hydrogen atoms within the matrix. In this contribution, the tensile property evolution of X52MS pipeline steel before and after hydrogen charging is investigated by combining electrochemical hydrogen charging test with slow stretching experiment. The results show that as the per-charging time increases, the number and size of hydrogen blisters rise, which is caused by hydrogen accumulation on the surface. For the test steel with the thickness of 7.1 mm, the hydrogen blister size reaches about 3 mm after 12 h of pre-charging, and the hydrogen embrittlement sensitivity index is the highest of 54.6%. In contrast, the test steel with the thickness of 6.3 mm has the lowest index of 14.7%, indicating the better resistance to hydrogen embrittlement. It can be concluded that the hydrogen blister size is positively correlated with the hydrogen embrittlement sensitivity index, and surface hydrogen accumulation is the key reason for hydrogen-induced crack initiation. Furthermore, the tensile strengths of the three test specimens change little after pre-charging, but the elongation gradually decreases. The shear lips on the side of the fracture are all featured by a zigzag shape, and the cracks appear in the necking area, with a relatively large fracture diameter, showing the obvious hydrogen damage features. The fracture center morphology gradually changes from dimple one to cleavage surface one after hydrogen charging. These insights provide theoretical basis and experimental guidance for the design and development of pipeline steel for hydrogen energy transportation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Jiuquan Iron and Steel (Group) Co., Ltd
Lanzhou University of Technology
Funding
the Science and Technology Project of Jiayuguan City · the Science and Technology Plan Project of Gansu Province
References (21)
Show source-provided references
1. 10.1016/j.ijhydene.2024.08.34110.1016/j.ijhydene.2024.08.341 ↗
2. Ren X, Chu W, Li J, et al. Influence of inclusions on initiation of hydrogen blister in iron. Acta Metall SINica 2007; 7: 673–677.
3. 10.1016/j.corsci.2008.09.01410.1016/j.corsci.2008.09.014 ↗
4. Liu T, Wei B, Fu A, et al. Hydrogen damage of X80 pipeline steel in hydrogen-doped gaseous atmosphere. J Chin Soc Corros Prot 2025; 45: 423–430.
5. Niu H, Li Y, Song W, et al. Slow strain rate tensile properties of X80 pipeline steel in different hydrogen-containing environments. Mater Mech Eng 2025; 49: 99–104.
6. Zhao Q, Liu H, Li M, et al. Study on the effects of partial pressure on X52M pipeline hydrogen embrittlement properties in high-pressure hydrogen environments. Spec Steel 2025; 46: 117–124.
7. 10.1016/j.ijhydene.2015.06.11110.1016/j.ijhydene.2015.06.111 ↗
8. Martin M Buck Z Eckhardt A et al. Effect of strain rate on tensile test results in hydrogen and other concerns [J]. Eng Fract Mech 2025 327: 111461.10.1016/j.engfracmech.2025.111461 ↗
9. 10.3390/met1506059610.3390/met15060596 ↗
10. 10.1016/j.corsci.2026.11362510.1016/j.corsci.2026.113625 ↗
11. Jiang X, Li Y, You J, et al. Multi-scale analysis and prospects of research on hydrogen embrittlement in metallic materials for hydrogen-related environments in modern chemical and energy processing. Clean Coal Technol 2025; 31: 125–141.
12. 10.3390/app1514781810.3390/app15147818 ↗
13. 10.1021/acsomega.5c0311110.1021/acsomega.5c03111 ↗
14. 10.3390/ma1824548710.3390/ma18245487 ↗
15. 10.1002/srin.20230037210.1002/srin.202300372 ↗
16. 10.1016/j.msea.2021.14204310.1016/j.msea.2021.142043 ↗
17. 10.1007/s11665-018-3556-710.1007/s11665-018-3556-7 ↗
18. Zhao X, Chen Y, Huang S, et al. Research on hydrogen diffusion in hot stamping steel and its relationship with hydrogen embrittlement layer. Die Mould Technol 2021; 4: 1–7.
19. Ren XC, Zhou QJ, Shan GB, et al. A nucleation mechanism of hydrogen blister in metals and alloys. Metall Mater Trans 2008; 87: 1543–1940.
20. 10.1016/j.ijhydene.2019.06.05410.1016/j.ijhydene.2019.06.054 ↗
21. 10.3390/met1407076310.3390/met14070763 ↗