To investigate the effect of DyCl 3 addition on the properties of micro-arc oxidation (MAO) coatings formed on TC11 titanium alloy, this study conducted MAO treatment in a silicate-phosphate composite electrolyte system with the introduction of DyCl 3 at different concentrations. By means of analytical equipment including scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), and an electrochemical workstation, the variations in the microstructure, phase composition, and corrosion resistance of the MAO coatings were studied. Results showed that with the addition of DyCl 3 , the final oxidation voltage was increased, the pore size of the MAO film was deceased, the surface roughness of the films was reduced, which means the denser and smoother MAO films. Dy 3 + participates in the film formation process in the form of the hard Dy 2 O 3 phase, which enhances the hardness and corrosion resistance of the coatings. Further analysis reveals that the MAO coating prepared when the DyCl 3 concentration is 0.15 g/L exhibits the optimal performance in key properties: its hardness and thickness reach 490.8 HV and 34.1 μm, respectively; in a 3.5% NaCl corrosive solution, it has the lowest corrosion rate of 2.9421 × 10 − 3 mpy, thus showing the best overall properties among all the prepared MAO coatings.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Titanium Alloys Microstructure and Properties · Bone Tissue Engineering Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Southwest Petroleum University
Sichuan-Chongqing Joint Key Laboratory of Green Hydrogen Production & Storage and Efficient Utilization, Chongqing, Sichuan, China
Xihua University
Funding
Key Laboratory of materials and surface technology, Ministry of Education
References (28)
Show source-provided references
1. 10.1016/j.apsusc.2025.16262010.1016/j.apsusc.2025.162620 ↗
2. Qiu GZ, Guo YF. Current Status review of corrosion resistance applications of titanium alloys in the petroleum industry. Coatings 2025; 14: 941.
3. 10.1177/0267084424127904110.1177/02670844241279041 ↗
4. 10.1088/1742-6596/2639/1/01205910.1088/1742-6596/2639/1/012059 ↗
5. 10.1016/j.identj.2024.07.113310.1016/j.identj.2024.07.1133 ↗
6. 10.1016/j.apsusc.2025.16387810.1016/j.apsusc.2025.163878 ↗
7. 10.1515/biol-2025-113210.1515/biol-2025-1132 ↗
8. 10.1016/j.surfcoat.2025.13246810.1016/j.surfcoat.2025.132468 ↗
9. 10.1111/ijac.1517710.1111/ijac.15177 ↗
10. 10.1016/j.vacuum.2025.11443510.1016/j.vacuum.2025.114435 ↗
11. 10.1016/j.matlet.2025.13893510.1016/j.matlet.2025.138935 ↗
12. 10.1016/j.ceramint.2014.12.13410.1016/j.ceramint.2014.12.134 ↗
13. 10.1177/0267083623121793110.1177/02670836231217931 ↗
14. 10.1080/02670844.2023.221294810.1080/02670844.2023.2212948 ↗
15. 10.1142/S0218625X1950093810.1142/S0218625X19500938 ↗
16. 10.1016/j.corsci.2025.11270610.1016/j.corsci.2025.112706 ↗
17. 10.1680/jsuin.22.0003310.1680/jsuin.22.00033 ↗
18. 10.1016/j.mtcomm.2025.11316810.1016/j.mtcomm.2025.113168 ↗
19. 10.1007/s12666-025-03607-w10.1007/s12666-025-03607-w ↗
20. 10.1016/j.jmrt.2022.09.11010.1016/j.jmrt.2022.09.110 ↗
21. 10.1016/j.ceramint.2023.08.03210.1016/j.ceramint.2023.08.032 ↗
22. 10.1016/j.tsf.2025.14070010.1016/j.tsf.2025.140700 ↗
23. 10.1016/j.jssc.2022.12351010.1016/j.jssc.2022.123510 ↗
24. 10.3390/ma1803072310.3390/ma18030723 ↗
25. 10.1007/s11665-023-08093-z10.1007/s11665-023-08093-z ↗
26. 10.1016/j.surfcoat.2025.13220610.1016/j.surfcoat.2025.132206 ↗
27. 10.1002/app.5681710.1002/app.56817 ↗
28. 10.1016/j.surfcoat.2025.13244510.1016/j.surfcoat.2025.132445 ↗