Material extrusion printing technology offers a reliable approach to low-cost additive manufacturing of metal materials. In this study, the debinding behaviour and binder composition of CuSn10 parts by material extrusion printing were investigated. The results showed that the binders were completely removed after the green parts were subjected to solvent debinding for 24 h and thermal debinding for 3 h. As the paraffin content rose, the feedstocks exhibited a reduction in viscosity accompanied by enhanced fluidity. The samples with 65 wt.% paraffin had the highest density, hardness and elongation of 7.677 g/cm 3 , 51.4 HB and 45.8%. The tensile strength reached the maximum value of 263.6 MPa with 70 wt.% paraffin.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Injection Molding Process and Properties · Additive Manufacturing and 3D Printing Technologies · Electronic Packaging and Soldering Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Hefei University of Technology
Research Center for Powder Metallurgy Engineering and Technology of Anhui Province, Hefei, China
Engineering Research Center of High Performance Copper Alloy Materials and Processing, Ministry of Education, Hefei, China
Funding
the Key Research and Development Program of Anhui Province, China
References (31)
Show source-provided references
1. Lu M, Shi X, Lu P, et al. Forming quality and wettability of surface texture on CuSn10 fabricated by laser powder bed fusion. AIP Adv 2023; 12: 125114.
2. 10.1016/j.jmrt.2025.03.08110.1016/j.jmrt.2025.03.081 ↗
3. 10.3390/met1111177410.3390/met11111774 ↗
4. 10.1016/j.jmrt.2024.06.11810.1016/j.jmrt.2024.06.118 ↗
5. 10.3390/ma1104061410.3390/ma11040614 ↗
6. 10.1016/j.jeurceramsoc.2023.09.07310.1016/j.jeurceramsoc.2023.09.073 ↗
7. Agarwala MK, Weeren R, Bandyopadhyay A, et al. Fused deposition of ceramics and metals: an overview. Proc Solid Free Fab Symp 1996; 47: 385–392.
8. 10.1016/j.ceramint.2022.06.15810.1016/j.ceramint.2022.06.158 ↗
9. 10.1016/j.ijrmhm.2025.10708810.1016/j.ijrmhm.2025.107088 ↗
10. 10.1016/j.ijrmhm.2023.10644510.1016/j.ijrmhm.2023.106445 ↗
11. 10.1108/RPJ-08-2023-026610.1108/RPJ-08-2023-0266 ↗
12. 10.1016/j.addma.2022.10267910.1016/j.addma.2022.102679 ↗
13. 10.1016/j.msea.2021.14141710.1016/j.msea.2021.141417 ↗
14. 10.1016/j.matdes.2022.11081410.1016/j.matdes.2022.110814 ↗
15. 10.1088/2631-8695/ad14af10.1088/2631-8695/ad14af ↗
16. 10.1016/j.jmapro.2024.05.00810.1016/j.jmapro.2024.05.008 ↗
17. 10.1016/j.addma.2022.10296610.1016/j.addma.2022.102966 ↗
18. 10.1007/s40964-024-00671-410.1007/s40964-024-00671-4 ↗
19. Côté R, Demers V, Demarquette NR, et al. A strategy to eliminate interbead defects and improve dimensional accuracy in material extrusion 3D printing of highly filled polymer. Addit Manuf 2023; 68: 103509.
20. 10.1016/j.ceramint.2023.05.01110.1016/j.ceramint.2023.05.011 ↗
21. 10.1080/00325899.2019.161613910.1080/00325899.2019.1616139 ↗
22. 10.1007/s00170-020-05323-910.1007/s00170-020-05323-9 ↗
23. 10.1007/s11665-024-09455-x10.1007/s11665-024-09455-x ↗
24. 10.1515/mt-2022-044310.1515/mt-2022-0443 ↗
25. 10.1177/0267083624124198610.1177/02670836241241986 ↗
26. 10.1016/j.powtec.2014.09.02010.1016/j.powtec.2014.09.020 ↗
27. 10.1016/j.msea.2005.06.05710.1016/j.msea.2005.06.057 ↗
28. 10.1557/PROC-542-13310.1557/PROC-542-133 ↗
29. Beran T, Mulholland T, Henning F, et al. Nozzle clogging factors during fused filament fabrication of spherical particle filled polymers. Addit Manuf 2018; 23: 206–214.
30. 10.3390/polym1417365310.3390/polym14173653 ↗
31. 10.1016/j.jmst.2023.12.04010.1016/j.jmst.2023.12.040 ↗