journal article·2025-10-15

Study on hot corrosion mechanism of nickel-base superalloy in molten NaCl-Na 2 SO 4 mixed salt

Qiu-hong Peng, Zhi-gang Sun, Xu-ming Niu

Publisher page

Abstract

In this study, GH4169 alloy(Corresponding to the US brand Inconel 718) was buried into NaCl-Na 2 SO 4 mixed salts to carry out hot corrosion. The image processing technology were employed to analyze the morphology of the corrosion layer, in order to reveal the hot corrosion mechanism of the alloy in molten salt. The results indicate that the crucible type and corrosion temperature have a great influence on the hot corrosion rate, corrosion surface morphology and formation mechanism of corrosion layer. The hot corrosion rate is mainly controlled by temperature, Al cation concentration in molten salt, stress in corrosion layer and other factors. The characteristic information extracted from the surface morphology after hot corrosion is closely related to the hot corrosion temperature and time.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Energy and Power Engineering, Nanjing University of Aeronautics and Astronautics

Key Laboratory of Aero-engine Thermal Environment and Structure, Ministry of Industry and Information Technology, Nanjing, PR China

Funding

National Science and Technology Major Project · National Natural Science Foundation of China · Postgraduate Research & Practice Innovation Program of Jiangsu Province

References (35)

Show source-provided references
1. 10.21533/pen.v3i1.4310.21533/pen.v3i1.43 ↗
2. 10.1016/j.engfailanal.2020.10438810.1016/j.engfailanal.2020.104388 ↗
3. 10.1007/s11085-020-09990-710.1007/s11085-020-09990-7 ↗
4. 10.1016/j.matpr.2017.11.36810.1016/j.matpr.2017.11.368 ↗
5. Simons EL, Browning GV, Liebhafsky HA. Sodium Sulfate in Gas Turbines. Corrosion -Houston Tx- 1955; 11.
6. 10.1007/BF0281326610.1007/BF02813266 ↗
7. Rizhang Z, Yu Z, et al. Investigation of the mechanism of internal sulfide internal oxidation during hot corrosion of nickel based superalloys. Acta Metallica Sinica 1985; 21: 39–116. (In Chinese).
8. 10.1016/S0010-938X(01)00057-910.1016/S0010-938X(01)00057-9 ↗
9. 10.1149/1.211410510.1149/1.2114105 ↗
10. 10.1002/maco.20130742510.1002/maco.201307425 ↗
11. 10.1007/s11085-013-9395-x10.1007/s11085-013-9395-x ↗
12. 10.1016/j.corsci.2023.11118610.1016/j.corsci.2023.111186 ↗
13. 10.1016/j.corsci.2022.11011310.1016/j.corsci.2022.110113 ↗
14. 10.1007/s11665-009-9399-510.1007/s11665-009-9399-5 ↗
15. Fei R, Weiwei W, et al. Theoretical calculation of saturated vapor pressure of pure water and construction of controllable water vapor generator . Laborat Res Explor 2016; 35: 56–59. (In Chinese).
16. 10.1016/j.solmat.2017.02.02010.1016/j.solmat.2017.02.020 ↗
17. 10.1016/j.pnsc.2021.04.00410.1016/j.pnsc.2021.04.004 ↗
18. 10.1007/s11665-021-05504-x10.1007/s11665-021-05504-x ↗
19. 10.1007/s11665-013-0532-010.1007/s11665-013-0532-0 ↗
20. 10.1016/j.jallcom.2018.01.04210.1016/j.jallcom.2018.01.042 ↗
21. 10.1007/s11665-018-3501-910.1007/s11665-018-3501-9 ↗
22. 10.1016/j.corsci.2019.04.02210.1016/j.corsci.2019.04.022 ↗
23. 10.1007/BF0104672710.1007/BF01046727 ↗
24. Yaru S, Shuai Z, Daile Z, et al. Effects of Cr, Al on hot corrosion behavior of low expansion Thermo Span superalloys. J Mater Res 2014(8): 6. (In Chinese).
25. Priymak EY, Gryzunov VI. Effect of temperature on the evolution of the process of oxidation of heating surfaces of tpp steam generators. Met Sci Heat Treat 2011; 52: 617–619.
26. 10.1155/2019/809721310.1155/2019/8097213 ↗
27. 10.1080/10408436.2016.124309010.1080/10408436.2016.1243090 ↗
28. 10.2320/jinstmet1952.61.1_5610.2320/jinstmet1952.61.1_56 ↗
29. 10.1520/MPC2020015610.1520/MPC20200156 ↗
30. 10.1016/j.matpr.2020.02.22610.1016/j.matpr.2020.02.226 ↗
31. 10.1016/j.corsci.2010.04.00710.1016/j.corsci.2010.04.007 ↗
32. 10.5006/1.357729110.5006/1.3577291 ↗
33. 10.1002/ceat.20090036510.1002/ceat.200900365 ↗
34. 10.1016/S0010-938X(03)00114-810.1016/S0010-938X(03)00114-8 ↗
35. 10.1007/s11085-006-9024-z10.1007/s11085-006-9024-z ↗