journal article·2026-07

Challenges for accurate and reliable determination of effective stress intensity factor range for structural assessments supporting incredibility of failure claims 1

Michael Nielsen

Materials Science and Technology· Volume 42· Issue 10
Publisher page

Abstract

Operation of a civil nuclear pressurised water reactor (PWR) facility results in a complex variable loading sequence arising from combined mechanical and thermal loadings, which must be evaluated in conjunction with welding residual stresses. This presents a challenge for fatigue crack growth (FCG) assessments at the design stage, with no load history, in support of a safety case for components where gross failure must be shown to be incredible within the design life. Assessment methods for FCG are generally contained within in-service inspection codes, e.g. RSE-M, ASME XI. The codified methods were not developed for use at the design stage and can be overly conservative as a result. This study considers the treatment of crack closure in the RSE-M code in the case of a low alloy steel component. The aim is to understand the reasonableness of the approach and if this assessment parameter is a potential source of significant conservatism. The primary focus is the treatment of the start-up/shutdown transients, with a negative R-ratio modified via the inclusion of welding residual stress. The study has been carried out using elastic-plastic cracked-body finite element models with a constant defect size i.e., propagation is not explicitly modelled. Crack growth is inferred by examination of behaviour ahead of the crack-tip and crack-tip opening displacement (CTOD) to determine an effective load range on an un-cracked elastic model to subsequently derive an effective stress intensity factor range ΔK .
Source: crossref · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · Structural Health Monitoring Techniques · Probabilistic and Robust Engineering Design

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Kinectrics

References (12)

Show source-provided references
1. AFCEN. RSE-M In-Service Inspection Installation and Maintenance Rules for Mechanical Components of PWR 2018 Edition.
2. Horn A James PM Nielsen MP et al. A review of the fatigue crack growth assessment approach to transient cycles and some of the other parameters used. TAGSI/P(23)222 Issue 1 2024.
3. Nielsen MP. An investigation of the rse-m crack closure parameter f(r) on a large ferritic pwr component with negative r-ratio including welding residual stress. In: Proc 9th Engineering integrity society international conference of durability and fatigue (Jesus College Cambridge UK June 2024) 2024 pp.506–519.
4. Walker K. The effect of stress ratio during crack propagation and fatigue for 2024-t3 and 7075-t6 aluminum. Effects of Environment Complex Load History Fatigue Life 1970: 1–14. doi: https://doi.org/10.1520/STP462-EB
5. ABAQUS. Version 6.14 analysis user’s manual dassault systemes simulia inc. 2014.
6. 10.1115/1.307839010.1115/1.3078390 ↗
7. Anderson TL. 2005.
8. Irwin GR. Analysis of stresses and strains near the end of a crack traversing a plate 1957.10.1115/1.4011547 ↗
9. Pellereau B Currie C Mann J et al. Investigation into crack closure effects for fatigue crack growth under negative r conditions. In: Proceeding of ASME 2020 pressure vessels & piping conference 2020 pp.PVP2020-21627 V001T01A022.
10. Watson C Currie C Emslie J. Accounting for negative r-ratio (crack closure) in fatigue crack growth calculations on stainless steel components. In: Proceeding of ASME 2015 Pressure vessels and piping conference July 19–23 2015 Boston Massachusetts USA 2015 pp.PVP2015-45622 V003T03A045;.
11. 10.1016/j.proeng.2010.03.19710.1016/j.proeng.2010.03.197 ↗
12. 10.3390/met1211185810.3390/met12111858 ↗