Influence of graphene on inclusions of slag–free self–shielded flux–cored arc welding layer
Source abstract
Abstract
The slag-free self-shielded flux-cored wire was modified by including graphene at concentrations of 0.00 wt.%, 0.15 wt.%, and 0.30 wt.%. The study's findings suggest that the primary constituents present in the deposited metal are AlN, Al 2 O 3 , Al 2 O 3 ·MgO, MgO, and MnS. The graphene reduces the average particle size from 2.59 μm to 2.13 μm as the graphene content increases. The inclusion 2 count reduces from 1599 to 1527 when graphene is introduced at a concentration of 0.30 wt.%. The fracture mode shown by the deposited metal is characterized by brittle fracture. Without graphene, the impact toughness value is measured to be 3.2 J/cm 2 . At a graphene addition of 0.3 wt.%, the impact toughness exhibits a rise to 7.2 J/cm 2 .
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Metal Alloys Wear and Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Material Science and Engineering, Hefei University of Technology, Hefei, China
School of Material Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang, China
Funding
Natural Science Foundation of Anhui Province · National Natural Science Foundation of China
References (21)
Show source-provided references
1. 10.1016/j.jmrt.2020.07.05210.1016/j.jmrt.2020.07.052 ↗
2. 10.1016/j.jmapro.2020.07.05610.1016/j.jmapro.2020.07.056 ↗
3. 10.1179/1362171815Y.000000005610.1179/1362171815Y.0000000056 ↗
4. 10.1016/j.surfcoat.2012.07.07810.1016/j.surfcoat.2012.07.078 ↗
5. 10.1016/j.ngib.2014.10.01510.1016/j.ngib.2014.10.015 ↗
6. Song SP, Li ZX, Li GD, et al. Effect of heat input on toughness of deposited metal at-40°C of self-shielded flux-cored wire. Adv Mat Res 2011; 291: 979–983.
7. 10.1016/S1002-0721(12)60180-X10.1016/S1002-0721(12)60180-X ↗
8. 10.1016/j.msea.2015.01.07010.1016/j.msea.2015.01.070 ↗
9. 10.1007/s12274-021-3345-810.1007/s12274-021-3345-8 ↗
10. 10.3390/met1208124710.3390/met12081247 ↗
11. 10.1016/j.jallcom.2017.05.15110.1016/j.jallcom.2017.05.151 ↗
12. 10.1007/s00419-017-1261-x10.1007/s00419-017-1261-x ↗
13. Zhu GY, Qin Y, Meng M, et al. Crossover between the adiabatic and nonadiabatic electron transfer limits in the Landau-Zener model. Nat Commun 2021; 12: 1–10.
14. Shuming X, Daben Z, Hanqi H, et al. Estimation of dendrite-to-granular transition time under continuous cooling and stirring. Chin J Nonferr Met 2001(S2): 234–237.
15. 10.1007/BF0054238410.1007/BF00542384 ↗
16. 10.1016/j.actamat.2018.11.02110.1016/j.actamat.2018.11.021 ↗
17. 10.1007/s11663-015-0568-710.1007/s11663-015-0568-7 ↗
18. 10.3389/fmats.2021.73628410.3389/fmats.2021.736284 ↗
19. 10.2355/isijinternational.ISIJINT-2021-03710.2355/isijinternational.ISIJINT-2021-037 ↗
20. 10.1088/1361-651X/ac969310.1088/1361-651X/ac9693 ↗
21. 10.1007/s11663-019-01532-010.1007/s11663-019-01532-0 ↗