Abstract

The interface formation and its mechanism of ZG42CrMo/BTMCr26 bimetallic castings, including hammerheads and thin plates, are investigated in this work. By extending the pouring interval, the interface area characteristic changes from local mixing solidification to shrinkage-filling solidification. Both interfaces exhibit high binding and tensile strength, exceeding 500 MPa. The casting bimetallic plates display a straight sequentially solidified interface with a carbide-free zone of approximately 16.5 μm. The interfacial adhesion and tensile strength of the plates also exceed 500 MPa. Based on the obtained results and theoretical basis, over 20 types of crusher hammers weighing between 7 and 250 kg, as well as various wear plates have been produced. Both castings exhibit high pass rate a long lifespan.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · High-Temperature Coating Behaviors · Materials Engineering and Processing

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering, Hebei University of Engineering, Handan, China

Hebei Key Laboratory of Wear-Resistant Metallic Materials with High Strength and Toughness, Hebei University of Engineering, Handan, China

Handan Huiqiao Compound Material Technology Co., Ltd, Handan, China

Center for Advanced Structural Materials, State Key Laboratory of Metastable Materials Science and Technology, Yanshan University, Qinhuangdao, Hebei, China

College of Mechanical and Equipment Engineering, Hebei University of Engineering, Handan, China

Handan Iron and Steel Group Co., Ltd, Handan, China

College of Materials Science and Engineering, Beijing University of Technology, Beijing, China

Handan Tianhao Wear-resistant Material Technology Co., Ltd, Handan, China

Funding

Hebei Province Technology Innovation Guidance program · Hebei Natural Science Foundation · Basic Research Project of Shijiazhuang City for Universities in Hebei Province

References (45)

Show source-provided references
1. 10.1016/j.trpro.2023.11.64110.1016/j.trpro.2023.11.641 ↗
2. 10.1016/j.cemconres.2022.10684210.1016/j.cemconres.2022.106842 ↗
3. 10.1016/j.scp.2024.10161110.1016/j.scp.2024.101611 ↗
4. 10.1088/1742-6596/1948/1/01218110.1088/1742-6596/1948/1/012181 ↗
5. 10.21833/ijaas.2019.02.01110.21833/ijaas.2019.02.011 ↗
6. 10.1016/j.matdes.2008.11.01510.1016/j.matdes.2008.11.015 ↗
7. 10.1016/j.wear.2017.01.02110.1016/j.wear.2017.01.021 ↗
8. 10.1016/j.triboint.2020.10671910.1016/j.triboint.2020.106719 ↗
9. 10.1016/j.matlet.2021.13141710.1016/j.matlet.2021.131417 ↗
10. 10.1016/j.jallcom.2020.15747210.1016/j.jallcom.2020.157472 ↗
11. 10.1016/j.wear.2018.04.00410.1016/j.wear.2018.04.004 ↗
12. 10.1016/j.wear.2023.20482810.1016/j.wear.2023.204828 ↗
13. 10.1007/s11661-006-0035-910.1007/s11661-006-0035-9 ↗
14. Fabián O, Dumitru F, Mesa D. Improvement of abrasive wear resistance of the high chromium cast iron ASTM A-532 through thermal treatment cycles. Revista Facultad De Ingenieria 2016; 25: 93–103.
15. 10.1016/j.mtcomm.2024.10849010.1016/j.mtcomm.2024.108490 ↗
16. 10.1016/j.vacuum.2023.11221810.1016/j.vacuum.2023.112218 ↗
17. 10.1016/j.msea.2018.01.11110.1016/j.msea.2018.01.111 ↗
18. 10.1016/j.jmrt.2020.05.01710.1016/j.jmrt.2020.05.017 ↗
19. 10.1016/j.triboint.2015.06.00210.1016/j.triboint.2015.06.002 ↗
20. 10.1016/j.matdes.2013.06.04510.1016/j.matdes.2013.06.045 ↗
21. Žic S, Džambas I, Ikonić MP. Possibilities of implementing bimetallic hammer castings in crushing industries. Metalurgija 2008; 48: 51–54.
22. 10.1016/S1006-706X(12)60145-910.1016/S1006-706X(12)60145-9 ↗
23. 10.1016/j.heliyon.2023.e1860710.1016/j.heliyon.2023.e18607 ↗
24. 10.1016/j.jallcom.2011.03.14210.1016/j.jallcom.2011.03.142 ↗
25. 10.1088/1757-899X/562/1/01203310.1088/1757-899X/562/1/012033 ↗
26. 10.1007/s40962-020-00532-010.1007/s40962-020-00532-0 ↗
27. Xiao X, Ye S, Yin W, et al. High Cr white cast iron/carbon steel bimetal liner by lost foam casting with liquid-liquid composite process. China Foundry 2012; 9: 136–142.
28. He L. The research on continuous core-filling casting forming process of copper-clad aluminum bimetal composite material. Acta Metallurgica Sin (English Lett) 2010; 23: 206–214.
29. 10.1016/j.wear.2017.02.00810.1016/j.wear.2017.02.008 ↗
30. 10.1016/j.matdes.2014.06.06710.1016/j.matdes.2014.06.067 ↗
31. 10.1007/s12666-021-02350-210.1007/s12666-021-02350-2 ↗
32. 10.1016/j.jmrt.2021.03.03210.1016/j.jmrt.2021.03.032 ↗
33. 10.1007/s12613-015-1154-310.1007/s12613-015-1154-3 ↗
34. 10.1016/j.matdes.2017.01.06610.1016/j.matdes.2017.01.066 ↗
35. 10.1016/j.msea.2020.13921310.1016/j.msea.2020.139213 ↗
36. 10.1016/j.jmatprotec.2018.06.01310.1016/j.jmatprotec.2018.06.013 ↗
37. 10.1016/j.matdes.2011.01.00610.1016/j.matdes.2011.01.006 ↗
38. 10.3390/ma1605200810.3390/ma16052008 ↗
39. 10.1088/2053-1591/ab637210.1088/2053-1591/ab6372 ↗
40. 10.1016/j.jmrt.2021.02.00710.1016/j.jmrt.2021.02.007 ↗
41. 10.1007/s11665-019-04401-810.1007/s11665-019-04401-8 ↗
42. 10.1002/srin.20210000110.1002/srin.202100001 ↗
43. 10.1016/j.vacuum.2023.11276510.1016/j.vacuum.2023.112765 ↗
44. 10.3390/ma1605200810.3390/ma16052008 ↗
45. 10.1016/j.matdes.2012.09.03710.1016/j.matdes.2012.09.037 ↗