ZK60 alloy deformation and damage at different temperatures using unified constitutive model
Source abstract
Abstract
The deformation behaviour and damage mechanism of ZK60 magnesium alloy under temperatures of 25–140 °C and strain rates of 0.01–0.0001 s −1 were investigated by uniaxial hot tensile and characterization experiments. The results suggested that the main factor for damage in ZK60 magnesium alloy was the nucleation, growth and coalescence of microdefects such as microvoids and cracks around the second-phase particles and/or grain boundaries. Then, a unified constitutive model including damage evolution, work hardening and recovery mechanisms was established. The model, verified by experimental data, shows good predictability. It was implemented into ABAQUS software through the VUMAT subroutine, which then predicted and analyzed the microstructure evolution.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metal Forming Simulation Techniques · Metallurgy and Material Forming · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Mechanical Engineering, University of Science and Technology Beijing, Beijing, People's Republic of China
Shunde Innovation School, University of Science and Technology Beijing, Foshan Guangdong, People's Republic of China
Beijing Key Laboratory of Lightweight Metal Forming, Beijing, People's Republic of China
Funding
National Natural Science Foundation of China
References (36)
Show source-provided references
1. 10.1080/02670836.2022.204307510.1080/02670836.2022.2043075 ↗
2. 10.1017/S143192761301222110.1017/S1431927613012221 ↗
3. 10.1016/j.jma.2017.09.00210.1016/j.jma.2017.09.002 ↗
4. 10.1016/j.matdes.2013.11.03710.1016/j.matdes.2013.11.037 ↗
5. 10.1016/j.ijplas.2021.10304010.1016/j.ijplas.2021.103040 ↗
6. 10.1016/j.jma.2017.09.00210.1016/j.jma.2017.09.002 ↗
7. 10.1016/j.jmrt.2023.11.20210.1016/j.jmrt.2023.11.202 ↗
8. Cockcroft MG. Ductility and workability of metals. J Metals 1968; 96: 2444.
9. 10.1016/0013-7944(85)90052-910.1016/0013-7944(85)90052-9 ↗
10. 10.1115/1.360120410.1115/1.3601204 ↗
11. 10.1299/jsme1958.15.150710.1299/jsme1958.15.1507 ↗
12. 10.1016/0022-5096(69)90033-710.1016/0022-5096(69)90033-7 ↗
13. Gurson AL. Continuum theory of ductile rupture by void nucleation and growth: part I-Yield criteria and flow rules for porous ductile media. J Eng Technol 1977; 99: 2–15.
14. 10.1016/0001-6160(84)90213-X10.1016/0001-6160(84)90213-X ↗
15. 10.1299/jsmea.45.9010.1299/jsmea.45.90 ↗
16. 10.1177/105678951350773110.1177/1056789513507731 ↗
17. 10.1016/j.jmatprotec.2016.09.00110.1016/j.jmatprotec.2016.09.001 ↗
18. 10.1016/j.msea.2017.12.02810.1016/j.msea.2017.12.028 ↗
19. 10.1007/s11665-022-07415-x10.1007/s11665-022-07415-x ↗
20. 10.3390/met1304074710.3390/met13040747 ↗
21. 10.1016/j.msea.2013.11.00810.1016/j.msea.2013.11.008 ↗
22. 10.1016/j.ijplas.2016.10.01110.1016/j.ijplas.2016.10.011 ↗
23. 10.1016/j.ijsolstr.2021.01.01310.1016/j.ijsolstr.2021.01.013 ↗
24. Xu S, Qian L, Ma T, et al. Investigation into the anisotropic damage behavior of LA103Z Mg-Li alloy rolling sheet using X-ray computed tomography and numerical modeling. Fatigue Fract Eng Mater Struct 2023; 27: 7368–7395.
25. 10.1016/j.actamat.2018.05.02610.1016/j.actamat.2018.05.026 ↗
26. 10.1007/s11661-020-05974-z10.1007/s11661-020-05974-z ↗
27. 10.1038/s41467-018-07028-w10.1038/s41467-018-07028-w ↗
28. 10.1177/105678950910348210.1177/1056789509103482 ↗
29. 10.1016/j.msea.2018.03.05010.1016/j.msea.2018.03.050 ↗
30. 10.1016/j.jma.2022.11.01310.1016/j.jma.2022.11.013 ↗
31. 10.1016/j.msea.2011.05.04710.1016/j.msea.2011.05.047 ↗
32. 10.1115/1.322577510.1115/1.3225775 ↗
33. 10.1177/105678950505035710.1177/1056789505050357 ↗
34. 10.1016/j.matdes.2015.06.09610.1016/j.matdes.2015.06.096 ↗
35. 10.1080/1478643041233130528510.1080/14786430412331305285 ↗
36. 10.1016/S0749-6419(99)00031-510.1016/S0749-6419(99)00031-5 ↗