Abstract

The effect of Sn content on the microstructure evolution of the as-cast, as-extruded and as-aged Mg-8Zn-2Y- xSn alloys were systematically investigated. The results show that addition of Sn not only refines the grains but also promotes the precipitation of quasicrystal I-phase and the formation of Sn 3 Y 5 . The phase transformations during solidification were also studied in detail. After extrusion, the broken second phase particles (I-phase) are more uniformly and densely distributed in the matrix with Sn addition. Moreover, ultra-fine dynamically recrystallized grains are obtained in extruded Mg-8Zn-2Y-0.5Sn alloy. In addition, high density nano-scale precipitates are uniformly dispersed by aging, and these precipitates are identified to be Mg-Zn particles, I phase and mixture of the [Formula: see text] Mg-Zn precipitates and I-phase.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloy Microstructure Properties · Quasicrystal Structures and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering, Chongqing University, Chongqing, People's Republic of China

National Engineering Research Center for Magnesium Alloys, Chongqing University, Chongqing, People's Republic of China

Funding

the National Key Research and Development Program of China

References (27)

Show source-provided references
1. 10.1016/j.msea.2019.13887710.1016/j.msea.2019.138877 ↗
2. 10.1016/j.matchar.2018.09.02110.1016/j.matchar.2018.09.021 ↗
3. 10.1016/j.matchar.2017.10.01710.1016/j.matchar.2017.10.017 ↗
4. 10.1016/j.scriptamat.2007.02.01510.1016/j.scriptamat.2007.02.015 ↗
5. 10.1088/1468-6996/15/2/02480110.1088/1468-6996/15/2/024801 ↗
6. 10.1088/0953-8984/20/31/31400110.1088/0953-8984/20/31/314001 ↗
7. 10.1016/j.scriptamat.2017.02.03910.1016/j.scriptamat.2017.02.039 ↗
8. 10.1016/j.msea.2011.05.00110.1016/j.msea.2011.05.001 ↗
9. 10.1016/j.msea.2011.01.10310.1016/j.msea.2011.01.103 ↗
10. 10.1016/j.matchar.2015.09.00510.1016/j.matchar.2015.09.005 ↗
11. 10.1016/j.msea.2013.06.00310.1016/j.msea.2013.06.003 ↗
12. 10.1016/j.scriptamat.2010.12.01610.1016/j.scriptamat.2010.12.016 ↗
13. 10.1007/BF0027707410.1007/BF00277074 ↗
14. 10.1016/j.jallcom.2015.07.25410.1016/j.jallcom.2015.07.254 ↗
15. 10.1016/j.msea.2016.10.03510.1016/j.msea.2016.10.035 ↗
16. 10.1016/j.msea.2017.11.04910.1016/j.msea.2017.11.049 ↗
17. 10.1557/JMR.2008.016610.1557/JMR.2008.0166 ↗
18. 10.1007/s13204-018-0854-110.1007/s13204-018-0854-1 ↗
19. Akhtar M · J Manuf Process · 2019 · 46 · 356
20. 10.1016/j.jallcom.2016.11.41310.1016/j.jallcom.2016.11.413 ↗
21. 10.1016/j.jallcom.2009.02.11910.1016/j.jallcom.2009.02.119 ↗
22. 10.1016/j.jallcom.2017.09.19210.1016/j.jallcom.2017.09.192 ↗
23. 10.1016/j.jallcom.2019.15312210.1016/j.jallcom.2019.153122 ↗
24. 10.1016/j.jallcom.2022.16396410.1016/j.jallcom.2022.163964 ↗
25. 10.1007/s10853-019-03460-510.1007/s10853-019-03460-5 ↗
26. 10.1007/s11661-013-2056-510.1007/s11661-013-2056-5 ↗
27. 10.1016/S0921-5093(03)00352-610.1016/S0921-5093(03)00352-6 ↗