Diamond fibres with soft ferromagnetic cores and a large magnetic shape anisotropy, were manufactured by chemical vapour deposition on to Fe and Fe-Cr steel wires. The wire cores were carburised during deposition and had a hardness of ∼550 kgf mm−2 (54 GPa). The fibres had an electrical resistivity of ∼ 153 μΩm and an elastic modulus of ∼ 600 GPa. Magnetic hysteresis loops (magnetisation v. applied field strength) and magnetic properties for the diamond fibres were compared with corresponding datafor Fe and Fe-Cr wires. The fibres may produce composites with a unique combination of properties.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced Surface Polishing Techniques · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (3)
Show source-provided references
1. 1994 · 10 · 505
2. 1996 · 5 · 65810.1016/0925-9635(95)00361-4 ↗
3. 1994 · 10 · 17710.1179/mst.1994.10.3.177 ↗