Superplastic behaviour of powder metallurgy 1.3%C-1.6%Cr-0.8%B steel
Source abstract
Abstract
The high temperature deformation behaviour of an ultrahigh carbon boron tool steel containing 1.3wt-%C-1.6wt-%Cr-0.8wt-%B was investigated. The steel was processed by powder metallurgy methods, involving argon atomisation and consolidation by hot isostatic pressing at 180 MPa for 2 h at 700°C. The microstructure of the consolidated material retains the dendritic solidification structure of the rapidly solidified powders. Aferritic grain size of 1 μm was measured. This steel presents a superplastic behaviour in the temperature range 660 to 1050°C with stress exponents of ∼2 at low strain rates and tensile elongations as high as 520% at 1000°C. A change in the activation energy at the α-γ transformation temperature (738°C) was clearly observed. The creep data are in agreement with grain boundary sliding and slip creep models.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Powder Metallurgy Techniques and Materials · Metal Alloys Wear and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. 10.1016/0036-9748(75)90352-X10.1016/0036-9748(75)90352-X ↗
2. 10.1007/BF0281201110.1007/BF02812011 ↗
3. 10.1007/978-1-4899-5880-810.1007/978-1-4899-5880-8 ↗
4. BUSBY P. E. · J. Met., · 1953 · 5 · 1463
5. GOLDSCHMIDT H. J. · J. Iron Steel Inst., · 1971 · 209 · 900
6. 10.1002/adma.1995007020510.1002/adma.19950070205 ↗
7. 10.1016/0921-5093(92)90403-N10.1016/0921-5093(92)90403-N ↗
8. BORLERA M. L. · Metall. Ital., · 1967 · 59 · 907
9. KOSTER W. · Z. Metallkd., · 1948 · 39 · 1
10. 10.1051/rphysap:0198800230406250010.1051/rphysap:01988002304062500 ↗