Crack propagation of secondary hardened alloy steels in gaseous hydrogen atmosphere
Source abstract
Abstract
The crack propagation behaviour of secondary hardened alloy steels having various Ni contents and a 18%Ni maraging steel was studied using modified compact tension specimens under 98–784 kPa hydrogen gas pressure pH2 . The effect of Ni content and retained austenite was examined by comparing oil quenched specimens with those cooled to liquid nitrogen temperature. It was estimated from the effect of pH2 on the crack propagation rate da/dt that the permeation of hydrogen from the crack tip surface decreased with increasing Ni content in the order 6 or 9, 13, then 18%Ni. It was also estimated that the hydrogen induced embrittlement of grain boundaries decreased with increasing Ni content in the order 6, 9, then 13%Ni and that the embrittlement was greater for the steel containing 18%Ni than for the steel containing 13%Ni. The effect of retained austenite was expected to suppress not the permeation of hydrogen, but the embrittlement of grain boundaries.MST/757
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. 10.1007/BF0264716810.1007/BF02647168 ↗
2. 10.1007/BF0264378810.1007/BF02643788 ↗
3. 10.1007/BF0264446210.1007/BF02644462 ↗
4. 10.1016/0036-9748(72)90126-310.1016/0036-9748(72)90126-3 ↗
5. 10.1007/BF0266422410.1007/BF02664224 ↗
6. 1975 · 31 · 40410.5006/0010-9312-31.11.404 ↗
7. 10.1007/BF0266738810.1007/BF02667388 ↗
8. 1970 · 1 · 63
9. 1976 · 110 · 30
10. 1975 · 9 · 43210.1179/030634575790444559 ↗