journal article·1997-07-01

Diamond fibre microheaters

P. G. Partridge, G. Meaden, E. D. Nicholson, J. A. Nicholson, M. N. R. Ashfold

Materials Science and Technology· Volume 13· Issue 7
Publisher page

Abstract

Free standing diamond fibres with 125 μm diameter tungsten wire or carburised steel cores coated by chemical vapour deposition with ∼ 35 μm thick diamond were heated by passing an electric current through the cores. Tungsten wire cored fibres were heated to 1000°C in a vacuum without any visible change in the fibres. In air the diamond oxidised above ∼550°C. The diamond fibres with the carburised steel core reached a maximum temperature of ∼ 200°C before melting at a local hot spot. This core was also ferromagnetic and thus the fibre had a unique combination of properties. Oxidation produced a large increase in the diamond surface area and this effect might be used to enhance heat transfer in diamond fibre sensors and in diamond fibre-metal matrix composite thermal conductors.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Metal and Thin Film Mechanics · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. 10.1016/0925-9635(94)05230-110.1016/0925-9635(94)05230-1 ↗
2. 10.1557/JMR.1995.144810.1557/JMR.1995.1448 ↗
3. 1997 · 13 · 453
4. 10.1557/JMR.1990.232010.1557/JMR.1990.2320 ↗
5. 10.1557/JMR.1990.248310.1557/JMR.1990.2483 ↗
6. 10.1007/BF0035399510.1007/BF00353995 ↗
7. 10.1007/BF0035598610.1007/BF00355986 ↗
8. 1994 · 10 · 505