Abstract
The 0.15C-1.5Mn and 0.07C-0.3Mo-0.055Nb steels were subjected to hot rolling to determine the effects on transformation to ferrite and to hot torsion to measure strength. After 25 or 50% reduction at 830°C, the acceleration during isothermal transformation in the range 700–600°C is much greater for C-Mn than for Mo-Nb; delays of 5–10 s before cooling reduce the acceleration markedly. In continuous cooling, three passes of 20% reduction raise the temperature of austenite decomposition, most noticeably at the higher rate 9 K S-l. At this rate, for the C-Mn the pearlite is refined and for Mo-Nb the promoted ferrite is refined more and enhanced over bainite than at lower rates. Intercritical rolling below Ar3 enhanced ferrite formation more in C-Mn in the range 780–720°C than in Mo-Nb over 750–690°C. The stronger Mo-Nb in torsion (900–1100°C, 0.1-5 S-l) exhibits an activation energy of 353 kJ mol-l compared with 316 kJ mol-l for C-Mn.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. 1977 · 12 · 24
2. 1979 · 47 · 998
3. 1971 · 2 · 1711
4. 1978 · 23 · 445
5. 1996 · 35 · 16910.1016/0008-4433(95)00046-1 ↗
6. 1991 · 30 · 11310.1179/cmq.1991.30.2.113 ↗
7. 10.1016/0924-0136(93)90078-K10.1016/0924-0136(93)90078-K ↗
8. 1991 · 7 · 81810.1179/026708391790185022 ↗
9. 1991 · 9 · 75
10. 1992 · 10 · 20710.1080/09603409.1992.11689420 ↗
11. 1979 · 3 · 120
12. 10.1016/0924-0136(95)01987-P10.1016/0924-0136(95)01987-P ↗
13. 10.1007/BF0266236410.1007/BF02662364 ↗
14. 10.1007/BF0265681410.1007/BF02656814 ↗
15. 1982 · 21 · 44510.1179/cmq.1982.21.4.445 ↗
16. 1987 · 39 · 28