journal article·1996-10-01

Microstructure and thermal stability of Al–Cr–X (X=Ni, Mo, Si) powders obtained by centrifugal atomisation

B. Sánchez, A. García-Escorial, M. C. Cristina, G. Caruana, M. Torralba

Materials Science and Technology· Volume 12· Issue 10
Publisher page

Abstract

The microstructure and the thermal stability of rapid solidified centrifugally atomised AI–3Cr–X (X=1Ni, 3Ni, 0·3Mo, 1Si, or 3Si, at.-%) powders were studied. Three main types of microstructure were observed in the powders: cellular, globular, and rosettelike. Some powders exhibited a mixture of these. In the atomised state the alloys usually had two phases, intermetallic Al13Cr2 and α-Al solid solution. Thermal stability was studied for a range of temperatures from 20 to 500°C. The phase Al3Ni appeared in the nickel containing alloys and grew upon heat treatment. The molybdenum containing alloy did not show any noticeable change upon heat treatment. With respect to the silicon containing alloys, the intermetallic Al13Cr2 transformed into Al13Cr4Si4 at high temperatures. On the basis of bibliographic information a nucleation map was calculated relating the prevalence of the intermetallic Al13Cr2 phase and the α-Al phase to the particle diameter and the chromium concentration of powder obtained by centrifugal atomisation.MST/3273
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Aluminum Alloys Composites Properties · Quasicrystal Structures and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (2)

Show source-provided references
2. 10.1007/BF0054792310.1007/BF00547923 ↗