Abstract

The wetting behavior of Cu-Ni-Ti brazing alloys on Si 3N 4 was investigated. The joining of Si 3N 4 to Si 3N 4 was carried out by using Cu-Ni-Ti brazing filler metal in different forms. The strength of Si 3N 4 / Si 3N 4 joints, brazed with brazing foils cut from the corresponding ingots melted under a vacuum, is not as high as expected. The causes were studied. The homogeneity of the brazing alloys was improved by using paste brazing filler. Concurrently, four brazing alloys with different compositions were newly designed, by which the maximum room temperature three point bend strength of Si 3N 4 / Si 3N 4 joint, 338.3 MPa, was obtained. The rapidly solidified brazing foils, with optimum compositions of Cu - Ni5 ~ 25-Ti16~28-B (at%), were also produced, thus the strength of Si 3 4 / Si 3N 4 joints being further increased to 402 M P a. The joining experiments of Si 3N 4 to 1.25 Cr ~ 0.5Mo steel were also performed. The ceramic/metal joints with high strength at both room temperature and high temperature of 723 K~773 K were achieved.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: 3D IC and TSV technologies · Electronic Packaging and Soldering Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.