article·2002-01-01

Effect of the addition of TiB_ 2 on mechanical properties of i-B-C composites

Baosheng Zhang

Abstract

TiB 2 /TiC ceramic composites were fabricated by Hot-pressed B 4 C and Ti powders(mole ratio1:3)under1800℃,35MPa conditions.The flexural strength and fracture toughness of composites were454MPa and8.4MPa·m 1/2 ,re spectively.When5%and20vol%TiB 2 are added,the rod-like particles appeared in composites.These particles are TiB 2 as confirmed by XRD.The flexural strength and fracture toughness of composites with5%TiB 2 particles were increased to540MPa and10.8MPa·m 1/2 ,respectively;but dropped to357MPa and8.19MPa·m 1/2 with20%TiB 2 .The microstructure of composites by the addition of TiB 2 was observed by means of SEM.The results show that the amount of rod-like particles TiB 2 with a length of10~40μm when5%TiB 2 is added is larger than that of20%TiB 2 composites and smaller amount of pores were observed when20%TiB 2 is added,lots of pores and some agglomerated TiB 2 grains were observed.These factors limited the rodlike TiB 2 growth and impaired the mechanical properties of composites.It is clear that in-situ formation of rod-like particles enhanced the composite properties with a definite content of TiB 2 ad-dition.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.