Influence of calculated purity of boron powder on TiB_2-Cu composites
Source abstract
Abstract
TiB2-Cu composites were fabricated by Self-propagating High-temperature Synthesis (SHS). The effects of four kinds of calculated purities of boron powder: 90%, 92%, 95% and 100%, on relative density, phase composition, microstructure, bending strength and fracture toughness of TiB2-Cu composites were studied. The results showed that the combination property of TiB2-Cu composites is the best when calculated purity of boron is 92%, not the actual purity of boron, which is 90%. Based on the principle that boron and oxygen impurity among the powders reacted to form volatile B2O3, two reasons from analysis can be obtained: the lower the calculation purity of boron is, the higher the actual content of boron and the impurity are. Higher impurity content can bring higher porosity. On the other hand, a little titanium dissolves into copper matrix at high temperature with the result that titanium is consumed and boron is residual. It is considered that calculation purity of boron should exceed its actual purity. Considering the combination effects of two reasons, the calculated purity of boron, of 92%, is the best one.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.