Effect of pre-oxidation on the microstructure of sintered SiC by PIM

Zhou Jie

Abstract

To investigate the effect of pre-oxidation on the microstructure of powder injection molded SiC,the moded green parts were debound in air furnace.Firstly,the porosity of sintered samples decreases with the pre-oxidation temperature increase from 550 ℃ to 650 ℃,and then increases from 650 ℃ to 950 ℃.The measured density of sintered sample with pre-oxidation at 650 is the largest(3.20 g/cm3) among all samples with or without pre-oxidation.Sintered samples contain SiC phase and intergranular liquid phase.There is no SiO2 in all sintered samples base on the analysis of XRD and TEM.The loss intergranular liquid phase affects the formation of YAG(Y3Al5O12).So,no diffraction peak of YAG is found in the test results by XRD.The average grain size of sintered samples is less than 1 μm.Test results indicate that,thermal debinding could be conformed in air instead of inert gas shield under 550~750 ℃.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.