Control mechanism and surface oxidation process optimization of cord wire steel
Source abstract
Abstract
Effect of finish rolling and spinning on thickness and phase composition of hot rolling wire rod surface oxide scale,continuous oxidation behavior under air atmosphere of cord wire steel was analyzed by means of Optical Microscope( OM),Scanning Electron Microscopy( SEM),and the conditions of proeutectoid and eutectoid transformation in FeO layer was analyzed by means of thermal simulation. The results indicate that 945 ℃ is the starting point of rapid oxidation,but the oxidation rate is very slow below 700 ℃. The cooling rate between 700 ~ 945 ℃ is the key process parameter of controlling thickness and phase composition of oxide scale. When the finish rolling and spinning are controlled in the range of 900 ~ 940 ℃,the oxide scale thickness is 7 ~ 20 μm and the FeO mass percent is 65% ~ 80%,which can meet the descaling performance. Thermal simulation results indicate that 400 ~ 500 ℃ is nose temperature of eutectoid transformation of which the incubation period is the shortest in FeO layer. The cooling rate in the range of 500 ~ 400 ℃ is the main method to inhibit eutectoid transformation in FeO layer,and the mechanical descaling rate can be increased by about 3%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.