article·2001-01-01

Preparation of long afterglow luminescence ceramic glaze brick with recycling waste glass and its properties

Wen Chang-ying

Abstract

SrAl 2O 4:Eu,Dy long afterglow luminescence powders were synthesized by the traditional ceramic preparing method. The main emission peak lies in a 520 nm wavelength, and the afterglow time was longer than 20 h. The long afterglow luminescence glaze was obtained by calcining the mixture of low melt point B-Si glass and SrAl 2O 4:Eu,Dy luminescence materials. Waste glass, small amount of additives and clay were used as the main raw materials of ceramic brick, and the low melting point luminescent glaze was coated on the ceramic brick. Finally, the long afterglow ceramic glaze brick can be fabricated under suitable synthesis conditions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.