Fracture toughness and toughening mechanisms of 3Y-TZP containing Al_2O_3 and mullite

LI Hong-xiangof

Abstract

The composites were prepared by a process of mixing 3Y-TZP, mullite and alumina by ball-milling, pressing unidirectionally, cold-pressing isostatically, and sintering in air. The composites with different fracture toughness were obtained by change of volume ratio of alumina to mullite. The compositions and microstructure of composites were examined by a X-ray diffractometer and a scanning electron microscope. The volume ratio of Al_2O_3 to mullite affected the transformable fraction of t-ZrO_2to m-ZrO_2, microstructure of the composites, and plane distance of t-ZrO_2, which lead to the difference of the fracture toughness. The fracture toughness of composites sintered at 1 480 ℃ for 4 hour in air was 9.26 ~10.4 MPa·m~(1/2) tested by the single-edge notched bending (SENB). In the composites, in addition to the contribution of the enhanced phase transformation, the dispersion-toughening of particles was also one of the main toughening mechanism.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicone and Siloxane Chemistry

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.