article·2001-01-01

Microstructure of Si_3N_4/Si_3N_4 joint brazed with (CuZn)_(85) Ti_(15) filling alloy

Jie Zhang

Abstract

The microstructure of the Si 3N 4/Si 3N 4 joint was investigated. The joint was made by active brazing using a filler of (CuZn) 85 Ti 15 alloy. A Si 3N 4/Si 3N 4 joint with a high bonding strength can be obtained with a suitable brazing condition. The joint layer is mainly composed of Cu 2TiZn and Cu solution with silicide and nitride containing Ti. With increasing welding temperature from 850 ℃, the thickness of the interfacial reaction layer increases and both amount and size of the reactant in the filling metal increase. The addition of Zn can decrease the melting point of the brazing alloy and the brazing temperature and as a result can improve the flowability and wettability of the brazing joint. The evaporation of Zn, which can be controlled by an appropriate brazing process, is enhanced with increasing welding temperature.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.