Effect of warm forming on the mechanical properties of AZ31 magnesium alloy

Baocheng Li

Abstract

Plane strain compression tests of different degrees of deformation at temperatures ranging from 210 to 300℃ were carried out for as - cast AZ31 magnesium alloy. The effect of warm forming on mechanical properties of AZ31 alloys was studied and analyzed according to the microstructure evolvement. Results showed that, at the same degree of deformation, the increment of tensible strength decreases with increasing temperature because the crystal grain becomes coarse; at the same temperature, the increment of tensible strength increases , gradually at first, with an increasing degree of deformation, but slightly decreases at a certain degree of deformation. High strength of 305 MPa was attained for AZ31 alloy at 210℃ when is 2.07. Compared with as - cast alloys, tensible strength enhanced about 50%. This suggests that fine grain and high strength are attained for AZ31 alloy by means of rational combined action of work hardening and fine grain strengthening during warm forming.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.