Failure analysis for the dissimilar metal joints of superheater tubes in power plant station

Meng Qing

Abstract

The dissimilar metal joints of superheater tubes cracked along the heat resistant steel HAZ after operating at high temperature for 4×10 4 hours at shen Tou ⅡPower Plant, and they cracked once again after being mended by arc welding and operating for a period of time. By means of fracture morphology and microstructure analysis, it is proved that the former failure is induced by creep damage, and can be explained by carbide concentration and carbon migration while the later failure is induced by SCC and it can be explained by stress and steam containing Cl -. Furthermore, the defects cause stress concentration and may induce SCC. Improving the welding process and using nickel based weld transition joint can improve creep strength and service life of A/F dissimilar metal joints.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.