article·2006-01-01

Effect of CuAl_2 dissolution during solution treatment on the strength of AlCu-Si alloys after aging

Dingfei Zhang

Abstract

After solution treated,Al-3.5Cu-7.0Si castings had obvious strength increase as solution time increasing.The first strength increase happens between 0 and 2 hours,with the increase range of Ultimate Tensile Strength(UTS) of 50 ~ 80 MPa compared with those of as-cast alloys,and the second happens between 4 ~ 8 hours,with the increase range of UTS about 20 MPa.Microstructure observations and SEM analyses showed that the first strength increase largely depended on the solution of fine CuAl_2 phases attached on some impurities and dispersed in the matrix,and also smoothed silicon particles after heating had a good effect on strength.The second one depended on the solution of blocky CuAl_2phase.Iron-rich compounds,especially β-FeSiAl_5 phase in the alloy,are very stable,which could not be dissolved or changed by normal solution treatment.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.