Dilatometry analysis of recovery characteristics in a Fe-17Mn- 10Cr-5Si-4Ni shape memory alloy
Source abstract
Abstract
The shape recovery characteristics in a Fe-17Mn-5Si-10Cr-5Ni shape memory alloy were studied using Formaster FTM-4 dilatometer. The continuous curves of strain recovery with heating temperature were accuratel plotted. The results show that for the fore and aft recovery of pre strained specimens, the expansion coefficient of alloy is nearly the same. The e→γ reverse martensitc transformation starting temperature As was independent of pre strain and the finishing temperature Af was increased with increasing pre strain. In process of recovery, the specimen recovers slowly at earlier and later stages, but in the middle stage the specimen recovers fast. The recovery ratio reduces with increasing pre strain and the maximum recovery strain is obtained when pre strain is about 5%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.