article·2000-01-01

Improvement of chemical stability of hollow glass microspheres by introducing Al_2O_3

Qiu Long

Abstract

Presents the process of adding Al 2O 3 up to mole ratio of 1.5% is introduced into HGM by complexing Al 3+ into glass forming solution, and fabricating HGM with different oxide ratios and outer diameter of 450~550 μm and wall thickness of 0.8~1.5 μm at higher fusing temperature of 1 400 ℃ and axial rate of purge gas up to 6~ 7 cm/s(25 ℃、0.101 MPa), and then washing the newly made HGM with 0.5MNH 4F+0.1MHNO 3 at 90 ℃, hot water and acetone for 5 min and twice, and then exposing the HGM to ambient air to trace the out surfaces by microscope and atomic force microscope (AFM) and concludes that the emerging of spots on the outer surfaces is delayed from 5 days to 20 days and the roughness increase rate is slowed down, and this shows that the chemical stability of the HGM is increased dramatically.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Photonic Crystals and Applications · Aerogels and thermal insulation · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.