article·2002-01-01

Effect of coating quantity of fluxes on weld penetration depth in A - TIG welding

Liqun Li

Abstract

Conventional TIG welding is known as its low productivity and limited weld depth in a single pass. Activating TIG welding (A - TIG) can greatly improve the weld penetration and thus enhance the process efficiency in comparison with the conventional TIG welding. The effect of fluxes with single component (SiO2、 CaF2 、TiO2 、Cr2O3 and NaF) on weld penetration by method of macro - section analysis during TIG welding of stainless steel has been investigated. The results show that compared with conventional TIG welding activating flux causes an enhancement in weld penetration and the enhancement increases with increasing coating quantity when the later is small. The increased weld penetration with oxide flux is the biggest, while the increased depth with fluoride flux is the smallest. However, each of these five types of flux has its saturation point in penetration increment. The arc constricting and the changing of weld pool surface tension gradient are the main reasons for the activating flux to increase the weld penetration.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Non-Destructive Testing Techniques · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.