Study on debinding process of injection molded tungsten heavy alloy feedstock
Source abstract
Abstract
The thermal debinding process parameters including sample thickness, pre-debinding at low temperature and temperature increasing schedule of injection molded tungsten heavy alloy power mixed with paraffin was based multi component binder system were studied and the experiments showed that the logarithm of weight loss was proportional to the reciprocal of sample thickness at temperature below 250 ℃, paraffin waxs can be removed thoroughly by long time debinding at 250 ℃. Inappropriate debinding parameters such as temperature increasing schedule can lead to debinding defects.