Fracture toughness of welded joints of A6005A aluminum alloy for high speed train
Source abstract
Abstract
To investigate the crack propagation of welded joints of A6005A aluminum alloy used in high speed train,a preliminary test is made to determine the fracture toughness and impact toughness.Three point belt and SEM has been used to test the fracture toughness CTOD δm(8)and Jm(8)of different regions of the welded joints.The results showed that the value of impact energy of HAZ was 16.3 J,the matrix was 11.5 J,and the weld was only 5.5 J.The δm(8) of HAZ was 0.373 9 mm,the matrix was 0.089 2 mm and the weld was 0.069 7 mm.The Jm(8) of HAZ was 109.454 kJ/m2,the matrix was 38.249 kJ/m2,and the weld was 16.231 kJ/m2..The dimples on the fracture surface of HAZ were larger than that on the matrix,which showed good toughness.The weld showed bad toughness and low impact energy because of the porosity and inclusions.The impact toughness and fracture toughness indicated the same rule that the HAZ zone had the best property in crack propagation,followed by the matrix and the weld.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fatigue and fracture mechanics · Advanced Welding Techniques Analysis · Engineering Applied Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.