article·1999-01-01

SiC_p-Al composites produced by pressureless infiltration and their abrasion resistances

Sheng Xu

Abstract

Studies the fabrication of SiC p/Al composite via pressureless infiltration with K 2ZrF 6 as an infiltration promoter. The effect of process factors, including ratio of K 2ZrF 6 and SiC p, SiC p size, preheating temperature for powder preform, pouring temperature of aluminium alloy melt, and soaking temperature and duration, were investigated. According to the metallographic analysis of composites, the optimum infiltration factors were determined which consist of a preheating of powder preform at 700 ℃, pouring and soaking aluminium alloy melt at 780~800 ℃, and a two hour soaking period followed by a cooling in the furnace. Experiments show that the hardness of the composites is 36%~58% higher than the matrix alloy and their abrasive resistances increase by 2~6 times.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.