Study of cold cracking sensibility of self-shielded flux cored arc welded U75V rail using implant test
Source abstract
Abstract
Implant tests were carried out to study the cold cracking sensibility of U75V steel welded by JDHS-38 # self-shielded flux cored wire.The influence of preheat temperature,heat input and number of weld passes on the critical press of U75V rail was studied.Results indicate that different methods should be taken to protect the HAZ from the influence of welding cold cracking,such as preheating the rail to 250 ℃,keeping heat input around 14 kJ/cm,using multi-layer welding method.Therefore,the critical fracture stress could reach 646 MPa,which is equivalent to its tensile stress.If adopting other processing parameters,the critical fracture stresses are much lower,and when the restraint stress is higher than tensile strength,the expiration break would happen in HAZ.The breaking nature is typical hydrogen-induced crack.The microstructures of superheat section are martensite and bainite,while the fracture appearances are mainly river pattern,pulpy pattern and ungular pattern.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.