Surface relief in dynamically embrittled low alloy steels with varied flow stress
Source abstract
Abstract
The dynamic embrittlement of low alloy steels with two different flow stresses at a low partial pressure of oxygen is presented. The low alloy steel with a higher flow stress experienced a relatively higher degree of dynamic embrittlement compared with the steel with a lower flow stress. Pronounced surface relief originated on the surface of intergranular facets, and is defined in terms of a surface deformation parameter determined from atomic force microscopy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Metal and Thin Film Mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. 10.1016/1359-6454(95)00249-910.1016/1359-6454(95)00249-9 ↗
2. 10.1016/0956-7151(90)90197-O10.1016/0956-7151(90)90197-O ↗
3. 10.1179/mst.1993.9.6.49710.1179/mst.1993.9.6.497 ↗
4. 10.1179/02670830422501661710.1179/026708304225016617 ↗
5. 10.1016/0956-716X(94)90058-210.1016/0956-716X(94)90058-2 ↗
6. 10.1016/S1359-6454(99)00117-210.1016/S1359-6454(99)00117-2 ↗
7. 10.1016/S1359-6454(01)00005-210.1016/S1359-6454(01)00005-2 ↗
8. 10.1016/0956-7151(94)00388-X10.1016/0956-7151(94)00388-X ↗
9. 10.1016/0956-7151(94)00387-W10.1016/0956-7151(94)00387-W ↗
10. 10.1016/0956-716X(92)90114-T10.1016/0956-716X(92)90114-T ↗
11. 10.1016/0001-6160(88)90018-110.1016/0001-6160(88)90018-1 ↗
12. 10.1016/0036-9748(86)90405-910.1016/0036-9748(86)90405-9 ↗
13. 10.1016/0956-7151(90)90252-C10.1016/0956-7151(90)90252-C ↗
14. 10.1016/0001-6160(84)90100-710.1016/0001-6160(84)90100-7 ↗
15. 10.1016/1359-6454(96)00109-710.1016/1359-6454(96)00109-7 ↗
16. 10.1016/1359-6462(96)00296-510.1016/1359-6462(96)00296-5 ↗
17. 10.1007/s11661-004-0045-410.1007/s11661-004-0045-4 ↗
18. 10.1016/j.msea.2003.10.20210.1016/j.msea.2003.10.202 ↗