Magnesium based Mg–9Al–1Zn–5RE (RE=Y, La, Nd, Ce, or Pr) alloys with or without an addition of 1%Si were rapidly solidified by chill block melt spinning and splat quenching. The base alloy AZ91 (Mg–9Al–1Zn) was also rapidly solidified. Isochronal heat treatment for 1 h at 100–400°C showed that the microhardness of the ribbon maintained a similar level to that of the as spun alloy up to 300°C but decreased when heat treated at 400°C. Isothermal heat treatment for up to 24 h at 250–350°C showed that there were aging responses for the sample treated at 250°C while above this temperature, the microhardness decreased as the treatment time increased. The addition of 5% of RE elements to AZ91 displaced the Mg17Al12 phase in AZ91 with fine dispersoids of Al2RE (RE=Y or Nd) or Al11RE3 (RE=La, Nd, Ce, or Pr) in Mg–9Al–1Zn–5RE alloys. These Al–RE intermetallics remained fine and precipitated at the grain boundaries so restraining grain growth during heat treatment at up to 400°C. Although Mg2Si precipitates were found to be present in the silicon containing alloys after heat treatment at 400°C, their size was greater than those of Al–RE intermetallics, indicating that Mg2Si has a lower thermal stability than these Al–RE intermetallics. The relationship between microhardness and grain size is discussed.MST/3400
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. 10.1007/BF0288216910.1007/BF02882169 ↗
2. 10.1007/BF0288216810.1007/BF02882168 ↗
3. 10.1007/BF0288316210.1007/BF02883162 ↗
4. 1989 · 9 · 44
5. 10.1007/BF0288316810.1007/BF02883168 ↗
6. 10.1016/0921-5093(91)90320-M10.1016/0921-5093(91)90320-M ↗