Microstructure and bond strength of Ni-Cr steel/Si3 N4 joint brazed with Ag-Cu-Zr alloy
Source abstract
Abstract
The interfacial microstructure and bond strength were examined for a Ni-Cr steel/Si3 N4 joint brazed using an Ag-Cu eutectic alloy containing 5 wt-%Zr. The reaction of Si3N4 with the brazing alloy formed a very thin ZrN layer with a cubic structure (a = 4.577 Å) at the interface. No Zr silicide (Zr5Si3) was present at the interface even though its formation is thermodynamically possible. The reaction product did not contain any of the dilute ceramic phases or intermetallics which are commonly seen in other active metal brazing systems. This strongly implies that the elements of the Ni-Cr steel and Ag or Cu in the brazing alloy, did not participate in the interfacial reaction. The shear strength of the joint was strongly dependent on the thickness of the reaction layer and the morphology of CuZr2 precipitates in the brazement. A joint with a reaction layer thickness of 0.5 μm, which was formed by brazing at 950°C for 30 min, showed the highest fracture shear strength (∼ 202 MPa).
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (8)
Show source-provided references
1. 10.1111/j.1151-2916.1993.tb03926.x10.1111/j.1151-2916.1993.tb03926.x ↗
2. 10.1007/BF0108212710.1007/BF01082127 ↗
3. 10.1007/BF0055131910.1007/BF00551319 ↗
4. 1986 · 2 · 115610.1179/mst.1986.2.11.1156 ↗
5. 10.1111/j.1151-2916.1990.tb06762.x10.1111/j.1151-2916.1990.tb06762.x ↗
6. 10.1111/j.1151-2916.1990.tb06552.x10.1111/j.1151-2916.1990.tb06552.x ↗
7. 10.1007/BF0035159610.1007/BF00351596 ↗
8. 10.1007/BF0059574310.1007/BF00595743 ↗