Effect of cooling rate on refining of primary silicon of hypereutectic Al-Si alloy

Wu Shu

Abstract

In this study the cooling rates of different samples have been measured, and the microstructure variations have been investigated with an Al-20%Si-1%Cu-0.5%Mg-0.5%Mn alloy under different refining treatments. The results show that, under different cooling rates in the range of 5 ℃/s to 100 ℃/s, the un modified alloy has very big primary silicon particles in the range of 50 μm to 120 μm, and the effect of cooling rate on primary silicon size is relatively remarkable. The variation of cooling rate has a relatively small effect on the refining of primary silicon with a phosphorous modification or a dual modifier. The dual modifier can modify eutectic silicon and primary silicon at the same time, and makes the primary silicon smaller than phosphorous modification. The primary silicon size can be reduced to less than 20 μm with the dual modifier.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Bauxite Residue and Utilization

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.