Effect of Ti on weld microstructure of PAW SiCp/Al MMCs
Source abstract
Abstract
SiC particle reinforced aluminum alloy matrix composite is welded by plasma-arc welding,under high temperature,matrix Al and reinforcement SiC generate interface reaction(3SiC+4Al=Al_4C_3+3Si) and form fragile phase Al_4C_3 which can reduce the mechanical performance of welding joint.So SiCp/6061Al is welded by plasma arc with alloying filler Ti and the ionized gas changed from simple Ar to N_2+Ar mixed in certain proportion.The effect of alloying filler Ti on the microstructure of welded joint is researched.The results show that the wettability between matrix Al and reinforcement SiC is improved,and interface reaction between reinforcement SiC and matrix Al is inhibited.New reinforcements of TiN、AlN are produced instead of harmful Al_4C_3 phases in the welded joint,so the mechanical performance of welded joint is obviously improved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.