journal article·1985-02

Simultaneous creep and oxidation of an Fe–5AL alloy at 973–1073 K

R. Rolls, C. S. Madueke

Publisher page

Abstract

Studies of the simultaneous creep and oxidation of an Fe-5Al alloy at constant stresses of 12 and 16 MN m−2 in the temperature range 973-1073 K have shown that the steady-state creep obeys a power law. The stress exponent n was found to lie between 5 and 7. The apparent activation energy for creep was in the range 77–397 kJ mol−1 and depended on the oxygen partial pressure Po2 of the test environment. The oxidation strengthening (steady-state creep rate ε decreasing) was found for an applied stress of 16 MNm−2 for Po2 in the range 10−7 to 1·013 × 105 Pa. At 12 MN m−2, strengthening occurred only in the range 973–1023 K; weakening was found at 1073 K. The primary causes of strengthening are believed to be the mechanical constraint of strongly adherent scales and internal oxide-dislocation interactions.MST/133
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. 10.1080/0141861810823955910.1080/01418618108239559 ↗
2. ROLLS R. · Metall. Trans., · 1983 · 14 · 1207
3. 10.1088/0022-3735/9/8/01010.1088/0022-3735/9/8/010 ↗
4. OIKAWA H. · Technol. Rep. Tohoku Univ., · 1982 · 47 · 67
5. 10.1080/0141861810823941910.1080/01418618108239419 ↗
6. F. GAROFALO: ‘Fundamentals of creep and creep-rupture in metals’, 81–83; 1965, New York, Macmillan.
7. ISHIDA Y. · Trans. AIME · 1966 · 236 · 964
8. 10.1179/msc.1978.12.2.10210.1179/msc.1978.12.2.102 ↗
9. LAWLEY A. · J. A. com., and B. W. CHAN · 1960 · 218 · 166
10. DAVIES R. G. · Trans. AIME · 1963 · 227 · 665