Transient liquid phase diffusion bonding of continuous SiC fibre reinforced Ti–6AI–4V composite to Ti–6AI–4V alloy
Source abstract
Abstract
A continuous SiC fibre reinforced Ti–6Al–4V composite was diffusion bonded in transient liquid phase to Ti–6Al–4V alloy plate using Ti–Cu–Zr amorphous filler metal. Joint strength increased with bonding time up to 1·8 ks and reached the maximum value of 850 MN m−2 which corresponded to 90% of the tensile strength of Ti–6Al–4V. The extent of deformation of Ti–6Al–4V in the vicinity of the bonding interface was small compared with that of solid diffusion bonding because of the low bonding pressure. The bonding layer had an acicular microstructure which was composed of Ti2Cu and α titanium with dissolved zirconium. Brittle products such as (Ti, Zr )5 Si3 or (Ti, Zr )5 Si4 were formed at the interface between the SiC fibres and the filler metal. These products existed only at the end of fibres, in very small amounts, therefore joint strength was not significantly affected by the products.MST/1989
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Titanium Alloys Microstructure and Properties · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. 10.1179/mst.1993.9.3.26410.1179/mst.1993.9.3.264 ↗
2. 10.1179/mst.1993.9.6.52010.1179/mst.1993.9.6.520 ↗
3. 10.2207/qjjws.5.20510.2207/qjjws.5.205 ↗
4. DUVALL D. S. · Weld. J. · 1974 · 203
5. 10.1111/j.1151-2916.1990.tb09799.x10.1111/j.1151-2916.1990.tb09799.x ↗
6. ENJO T. · J. Jpn Inst. Met., · 1980 · 44 · 65910.2320/jinstmet1952.44.6_659 ↗