Environmental embrittlement of Al–Sn alloys and its implication for fatigue crack growth

A. K. Busby, J. W. Martin, N. J. H. Holroyd

Publisher page

Abstract

The environmental embrittlement of a series of Al–Sn alloys has been studied using the technique of slow strain rate testing in laboratory air, in a packing of anhydrous magnesium perchlorate, and in a salt solution (2%NaCl–0·5%Na2CrO4 buffered to pH 3·5). The embrittlement occurring at slow strain rates is attributed to reversible hydrogen embrittlement. Only the alloy containing a continuous network of tin phase suffers a reduction in ductility. This is attributed to an increase in hydrogen diffusivity which is demonstrated through a series of permeation tests. These results are then used to interpret fatigue crack growth tests conducted as a function of environment in the absence of closure.MST/744
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (6)

Show source-provided references
1. 10.1179/imr.1973.18.2.6210.1179/imr.1973.18.2.62 ↗
2. 10.1007/BF0240324810.1007/BF02403248 ↗
3. PARKINS R. N. · Stress corrosion cracking — the slow strain rate technique', STP 665,
4. N. J. H. HOLROYD and G. M. SCAMANS: ‘Environment-sensitive fracture: Evaluation and comparison of test methods’, STP 821, 202; 1984, Philadelphia, PA, ASTM.10.1520/STP34434S ↗
5. N. J. H. HOLROYD and D. HARDIE: ‘Effect of hydrogen on the behaviour of materials’ (Conf. Proc.), 449; 1981, New York, AIME.
6. 10.1111/j.1365-2818.1981.tb01305.x10.1111/j.1365-2818.1981.tb01305.x ↗