Effects of KOH/MMB weight ratio on structure and morphology of activated mesophase carbon microbeads
Source abstract
Abstract
In order to prepare the high surface area activated mesocarbon microbeads with high mesopore content, mesophase pitch microbeads were activated with KOH at 850 ℃ and the effects of the weight ratio of KOH/MMB to the structure and morphology of activated carbon microbeads were investigated in this paper. Both the total pore volume and the mesopore volumetric proportion of activated carbons increase with increasing the weight ratio KOH/MMB to a maximum, and then decrease with further increase of the weight ratio. The activated mesocarbon microbeads with the highest BET surface area (3 182 m2/g), the highest pore volume (245 cm3/g), and large percentage (62%) of mesopore volume were prepared with the KOH/MMB ratio of 8. With the increase of KOH/MMB ratio from 8 to 10, the total pore volume and surface area decrease to 239 cm3/g and 2 548 m2/g respectively, but the mesopore volume reach the highest value of 157 cm3/g. The results also indicate that, with increasing KOH/MCMB weight ratio, the sizes of the activated carbon microbeads can be reduced and the forms of the activated carbon microbeads change from sphere to ellipsoid, and then become smaller beads. On basis of the above results, the activation mechanism of MMB with KOH was discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Fiber-reinforced polymer composites · Polymer composites and self-healing · Electrospun Nanofibers in Biomedical Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.