Effect of pressing temperatures on strength of Al85La1 0Ni5alloys
Source abstract
Abstract
Using a powder hot pressing technique, high strength Al85La10Ni5 alloy specimens of size 20 (dia.) × 10 mm have been obtained under certain conditions. The pressing conditions for the alloy with the optimum mechanical properties are: temperature 753-853 K, time 15 min, and stress 1.2 GPa. The high strength of the alloy is attributed to second phase strengthening and fine grain strengthening. The highest ultimate compressive strength is 950 MPa at pressing temperature 773 K.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Quasicrystal Structures and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. 10.1038/341183a010.1038/341183a0 ↗
2. 10.1016/S0079-6425(98)00005-X10.1016/S0079-6425(98)00005-X ↗
3. WATANABE M. · Mater. Trans JIM · 1993 · 34 · 162 — 168
4. 10.2320/matertrans1989.37.128710.2320/matertrans1989.37.1287 ↗
5. JIANG Q. · Mater. Sci. Technol · 1997 · 13 · 284
6. ZHAO M. · Trans Nonferrous Met. Soc. China · 1999 · 9 · 48
7. 10.1179/00325890222500248810.1179/003258902225002488 ↗
8. 10.1007/s11661-000-1019-910.1007/s11661-000-1019-9 ↗
9. 10.1103/RevModPhys.71.173710.1103/RevModPhys.71.1737 ↗