Strength, toughness, and stiffness of wrought and directly sintered T6 high-speed steel at 20–600°C

P. W. Shelton, A. S. Wronski

Publisher page

Abstract

The mechanical properties of directly sintered T6 high-speed steel in the temperature range 20–600°C were generally comparable to those of concurrently heat-treated wrought material of similar composition. For the hardness range 860–940 HV30 macroscopic ductility was detected at 200°C and 450°C in the wrought and sintered materials, respectively; failure strains, however, did not exceed 2%. The value of Young's modulus dropped from ∼240 to ∼120 GNm −2 as the temperature was raised to 600°C, yield strength dropped from 2·2 to 1·0 GNm −2 , but the fracture strengths showed a maximum, ∼2·1 GNm −2 at ∼400°C for the wrought steel and ∼1·4 GNm −2 at ∼450°C for the sintered steel. Microcracking preceded yielding and/or failure and was mainly through carbides, which were generally below the critical size to cause catastrophic fracture. The second stage of the failure process involved the linking through the matrix of such microcracks until conditions for fast fracture were satisfied (stage three). A quantitative model for carbide cracking in high-speed steels is absent as is the correlation of fracture strength with fracture toughness via the critical defect size, since, for example, the failure originating zones in wrought samples identified by scanning electron microscopy were generally larger than those predicted by linear elastic fracture mechanics (LEFM). It is suggested that there may be some analogies between failure in monotonic loading of high-speed steels and of ceramics with small defects; the behaviour in fatigue of short cracks in alloys and microscopic crack growth in delayed fracture of ceramics where LEFM analyses developed as a result of studying artificial long cracks appear not to hold. MST/606
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Powder Metallurgy Techniques and Materials · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. JAGGER F. L. and PRICE W. J. C.: in Proc. 3rd European Powder Metallurgy Symposium (Powder Metall. Conf. Suppl.) 1971 Part 1 407–424.
2. JAGGER F. L. WALKER P. I. and PRICE W. J. C.: in Proc. 5th Int. Conf. on ‘Powder metallurgy’ Oct. 1978 Gottwaldov Czechoslovakia Czechoslovak Academy of Science Vol. 2 257-272.
3. DICKINSON E. A., and WALKER P. I.: Met. Powder Rep., 1980, 35, 18–20.
4. SMITH A. B. and WHITTLE N. C.: in Proc. 25th Int. Machine Tool Design and Research Conf. (ed. Tobias S. A.) 261; 1985 London Macmillan.
5. CLARK J. C.: in Proc. 21st Joint Propulsion Conference July 1985 Monterey Cal. AIAA/SAE/ASME/ASEE p. 1-7.
6. 10.1007/BF0281198210.1007/BF02811982 ↗
7. 10.1007/BF0267033010.1007/BF02670330 ↗
8. BROWN P. F. Jr G. A. BOGARDUS R. D. DAYTON and D. S. sctruLze: in ‘Rolling contact fatigue testing of bearing steels’ STP 771 (ed. Hoo J. J. C.) 323-341; 1982 Philadelphia Pa American Society for Testing and Materials.10.1520/STP36147S ↗
9. BAMBURGER E. N.: in ‘Tribology in the ‘80s’ 773-793; 1983 Washington DC NASA.
10. WRONSKI A. S. HUSSAIN AL-YASIRI L. B. and JAGGER F. L.: Powder Metall. 1979 22 109–118.10.1179/pom.1979.22.3.109 ↗
11. ERIKSSON K.: Scand. J. Metall., 1975, 4, 182–184.
12. SHELTON P. W. and WRONSKI A. S.: in ‘Towards improved performance of tool materials’ (ed. Irani R. S. et al.) 176–182; 1982 London The Metals Society.
13. SHELTON P. W.: PhD thesis University of Bradford 1985.
14. 10.1179/03063458379042046610.1179/030634583790420466 ↗
15. sisco F. T.: ‘The alloys of iron and carbon’ Vol. 2 1937 New York McGraw Hill.
16. NADAI A.: ‘Theory of flow and fracture of solids’ Vol. 1 2 edn 363-366; 1950 New York McGraw-Hill.
17. 10.1115/1.364064910.1115/1.3640649 ↗
18. 10.1007/BF0266157010.1007/BF02661570 ↗
19. 10.1007/BF0114063010.1007/BF01140630 ↗
20. 10.1111/j.1151-2916.1983.tb10537.x10.1111/j.1151-2916.1983.tb10537.x ↗
21. 10.1115/1.322561310.1115/1.3225613 ↗
22. 10.1111/j.1460-2695.1982.tb01250.x10.1111/j.1460-2695.1982.tb01250.x ↗
23. FINE M. E. and RITCHIE R. O.: in ‘Fatigue and microstructure’ 245-278; 1979 Metals Park Ohio American Society for Metals.
24. 10.1179/msc.1979.13.6.34110.1179/msc.1979.13.6.341 ↗
25. 10.1111/j.1151-2916.1973.tb12438.x10.1111/j.1151-2916.1973.tb12438.x ↗
26. 10.1007/BF0266330210.1007/BF02663302 ↗
27. WRONSKI A., and PINEAU A.: submitted to Int. J. Fract.
28. BEISS P. WAHLING R. and DUDA D.: in ‘Modern developments in powder metallurgy’ Vol. 17 331-357; 1985 Princeton NJ Metal Powder Industries Federation.
29. RICE R. W.: in Tractography of ceramic and metal failures’, (ed. Mecholsky J. J. and S. R. Powell, Jr), 5-103; 1984, Philadelphia, Pa, American Society for Testing and Materials.
30. JEANDIN M., , AUBIN C., , and BIENVENU Y.: Met. Powder Rep., 1982, 37, 187–190.
31. OLIVEIRA M. M. MARTINS I. M. MESQUITA R. M. M. B. MARQUES and II. CARVALHINHOS: in ‘Horizons of powder metallurgy’ (ed. Kaysser W. A. and Huppmann W. J.) 233-235; 1986 Freiburg Verlag Schmid.