Investigation of mechanical properties of advanced Al–Zn–Mg–Cu alloy
Source abstract
Abstract
The mechanical properties of the rapidly solidified 7000 series powder alloy CW 67 were investigated for various extrusion and heat treatment conditions. The principal aim of the work was to ascertain the optimum processing route for peak aged (T6) material. The highest proof stress in the T6 condition was found to be 572 MN m −2 for material extruded at 325°C and aged for 13·5 h at 120°C after solutionising. The ductility of this material was found to be 13·5%. The fracture toughness was measured in two orientations and found to be approximately 21 MN m −3/2 in the short transverse direction and 44 MN m −3/2 in the longitudinal direction. Degassing and hot compaction was found to improve the fracture toughness of the material substantially. MST/1504
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. HILDEMAN G. J. LABARRE L. C. HAFEEZ A. and ANGERS L. M.: in Proc. Symp. on ‘High strength powder metallurgy aluminium alloys’ 25; 1985 Warrendale PA The Metallurgical Society of AIME.
2. DAVIES C. H. J. RAGHUNATHAN N. and SHEPPARD T.: Mater. Sci. Technol. 1992 8 (11) to be published.10.1179/026708392790409798 ↗
3. ‘Metals handbook’ 9 edn Vol. 4 681 682; 1992 Materials Park OH ASM.
4. 10.1016/0013-7944(77)90028-510.1016/0013-7944(77)90028-5 ↗
5. 10.1016/0013-7944(84)90017-110.1016/0013-7944(84)90017-1 ↗
6. ‘Aluminium — properties and physical metallurgy’ (ed. Hatch J. E. ); 1984 Metals Park OH ASM.
7. 10.1007/BF0061147310.1007/BF00611473 ↗
8. THACKERY P. A.: J. Inst. Met., 1968, 96, 228.
9. 10.1007/BF0291340310.1007/BF02913403 ↗
10. 10.1007/BF0265471310.1007/BF02654713 ↗
11. FINK W. L., and WILLEY L. A.: Trans. AIME, 1948, 175, 414.