Cooling behaviour and microstructure of rapidly solidified Ag-Cu alloys
Source abstract
Abstract
A systematic experimental approach has been used to study rapid sotidification of Ag-Cu alloys with 23, 28.1 (eutectic), and 33 wt-%Cu using a levitation casting technique. The cooling curves were recorded during each experimental run and the microstructure was examined. Different cooling rates were obtained ranging from 3.2 × 104 to 10 × 104 K S-l, with nucleation undercoolings of 35–132 K, while growth undercooting was in the range 12–52 K. Under these conditions, the microstructure did not exhibit any lamellar structure. Instead, several other structures were obtained mainly, microsegregationfree, banding, columnar, and equiaxed dendritic structures. A correlation was made between each type of structure, the cooting rate, and the nucleation undercooling. The results are discussed and compared with previous work.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Solidification and crystal growth phenomena · Aluminum Alloy Microstructure Properties · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. 1994 · 197 · 587
2. 10.1016/0921-5093(91)90973-Q10.1016/0921-5093(91)90973-Q ↗
3. 10.1007/BF0264326410.1007/BF02643264 ↗
4. 10.1016/0001-6160(89)90277-010.1016/0001-6160(89)90277-0 ↗
5. 10.1007/BF0073847710.1007/BF00738477 ↗
6. 10.1007/BF0264438710.1007/BF02644387 ↗
7. 10.1007/BF0056625010.1007/BF00566250 ↗
8. 1992 · 40 · 983
9. 10.1016/0001-6160(69)90116-310.1016/0001-6160(69)90116-3 ↗
10. 10.1063/1.32986710.1063/1.329867 ↗
11. 10.1016/0001-6160(76)90108-510.1016/0001-6160(76)90108-5 ↗
12. 10.1007/BF0264511010.1007/BF02645110 ↗
13. 10.1016/0001-6160(77)90240-110.1016/0001-6160(77)90240-1 ↗
14. 10.1016/0022-0248(83)90179-310.1016/0022-0248(83)90179-3 ↗
15. 10.1016/0001-6160(86)90131-810.1016/0001-6160(86)90131-8 ↗
16. 1990 · 38 · 2683