journal article·1997-02-01

Stepped austempering heat treatment of a 0-67%Mn-Mo-Cu ductile iron

H. Bayati, R. Elliott

Materials Science and Technology· Volume 13· Issue 2
Publisher page

Abstract

Measurements of the retained austenite content, average austenite C content, UTS, 0.2% proof strength, elongation, and unnotched Charpy impact energy are reported for the stepped austempering treatment (870°C for 120 min; 375°C for 120 min; 285°C)as a function of austempering time at 285°C for a ductile iron of composition Fe–3.5 C–2.64Si–0.67n–0.007P–0.013S–0.25Mo–0.25Cu–0.04Mg (wt-%). These measurements are compared with previous measurements for single and stepped austempering treatments. The comparison shows that stepped austempering treatments can be used to improve elongation and impact energy obtained in single treatments in the high Mn ductile iron. Control over the austenitising and first step austempering temperatures can be used to change the relative improvements in elongation and impact energy. The austempering time required to achieve these improvements is much longer than that used in a single step treatment.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. 1995 · 11 · 118
2. 10.1179/02670830112500018610.1179/026708301125000186 ↗
3. 1993 · 9 · 882
4. 1993 · 9 · 586
5. 1995 · 11 · 1007
6. 1995 · 11 · 908
7. 1995 · 11 · 776
8. 1995 · 11 · 293